MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Thermx® TE4005 PCT, 33% Mineral / Glass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polycyclohexylenedimethylene Terephthalate (PCT); Polycyclohexylenedimethylene Terephthalate (PCT), Glass/Mineral Reinforced

Material Notes: Thermx« TE4005 NC010 is a 33% glass fiber/mineral reinforced polycyclohexylenedimethylene terephthalate resin developed for injection molding applications. It is specifically suitable for high performance demainding ignition applications. PRELIMINARY DATA

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0028 cm/cm0.0028 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0052 cm/cm0.0052 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 110 MPa16000 psi5mm/min; ISO 527-2/1A
Elongation at Break 1.8 %1.8 %5mm/min; ISO 527-2/1A
Tensile Modulus 9.00 GPa1310 ksi50mm/min; ISO 527-2/1A
Charpy Impact Unnotched 4.00 J/cm²19.0 ft-lb/in²ISO 179/1eU
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 46.0 kV/mm1170 kV/inIEC 60243-1
 
Thermal PropertiesMetricEnglishComments
Melting Point 285 °C545 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 230 °C446 °FISO 75-1, -2
 
Processing PropertiesMetricEnglishComments
Processing Temperature 120 - 140 °C248 - 284 °Fcavity
Melt Temperature 295 - 310 °C563 - 590 °F
Drying Temperature 95.0 °C203 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour
Moisture Content <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Thermx® TE4004 PCT, 40% Specialty

PHCQ472 / 178927

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.