MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont™ Clysar® LLP Polyolefin Shrink Packaging Film, 75 Gauge  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyolefin; Polyolefin, Film Grade; Polyolefin, Film Grade (Polyolefin)

Material Notes: Data provided by DuPont Packaging Polymers.

A strong, clear, biaxially oriented, nonirradiated, heat-shrinkable, linear low-density polyolefin film. LLPS is the silicon treated, hot slip version of LLP. Used where excellent optics and a tough, durable wrap are required. Ideal for low profile, long products. Strong seals and excellent shrinkage are obtained with all gauges. This is the fastest sealing linear low-density shrink film.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Moisture Vapor Transmission 0.510 cc-mm/m²-24hr-atm1.30 cc-mil/100 in²-24hr-atmASTM 1249
Water Vapor Transmission 27.0 g/m²/day1.74 g/100 in²/dayASTM 1249
Oxygen Transmission 148 cc-mm/m²-24hr-atm376 cc-mil/100 in²-24hr-atmor 7800 cc/m²-24hr-atm for the film. ASTM D3985
Thickness 19.0 microns0.750 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 135 %135 %Average; ASTM D882
Modulus of Elasticity 0.410 GPa59.5 ksi(stiffness), ASTM D882
Impact Test 1.40 J1.03 ft-lbSpencer Impact ASTM D3420
Coefficient of Friction, Dynamic 0.200.20ASTM D1894
Elmendorf Tear Strength MD 25 g25 gOrientation not specified; ASTM D1922
Film Tensile Strength at Break, MD 103 MPa14900 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 1.5 %1.5 %
Gloss 145 %145 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Hifax™ CB285 Thermoplastic Polyolefin Elastomer
ExxonMobil Label-Lyte™ 50TD200 OPP Film
RheTech Products FT1002-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Sumitomo Bakelite RX® 1310 Diallyl Ortho-Phthalate Molding Compound
Cosmic Plastics 306 Orlon Filled Diallyl Iso-Phthalate Molding Compound

PDU764 / 33180

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.