MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M Nextel™ 720 Composite Ceramic Fiber
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide; Other Engineering Material; Composite Fibers

Material Notes: Chemical composition above is wt%. Filament diameter is 10-12 µm.

3M Nextel Ceramic Fibers 610, 650, and 720 are composite grade fibers. They have a refined crystal structure based on alpha-Al2O3 and do not contain glassy phases. This allows the fibers to retain their strength at high temperatures. 3M Nextel Fiber 720, an alpha-Al2O3 with SiO2 addition (forming alpha-Al2O3/mullite), has improved strength retention at temperature due to reduced grain boundary sliding. The SiO2 addition also help to 'pin' the grains and reduce grain growth when exposed to thermal aging.

Information provided by 3M Ceramic Textile and Composites.

Key Words: Alumina, Aluminum Oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.40 g/cc0.123 lb/in³
Particle Size <= 0.50 µm<= 0.50 µmCrystal size
Specific Surface Area <= 0.20 m²/g<= 0.20 m²/g
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 2100 MPa
@Thickness 25.4 mm
305000 psi
@Thickness 1.00 in
gauge filament
Tensile Modulus 260 GPa37700 ksiFilament property
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.00 µm/m-°C
@Temperature 100 - 1100 °C
3.33 µin/in-°F
@Temperature 212 - 2010 °F
Melting Point 1800 °C3270 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.671.67
 
Descriptive Properties
ColorGreen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Nextel™ 312 Industrial Ceramic Fiber
3M Nextel™ 610 Composite Ceramic Fiber
3M Nextel™ 550 Industrial Ceramic Fiber
3M Nextel™ 440 Industrial Ceramic Fiber
3M Nextel™ 650 Composite Ceramic Fiber

CMMM06 / 1617

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.