MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI adhesives

SABIC LEXAN™ Healthcare HPS4 PC (Asia)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Gamma Radiation Resistant

Material Notes: Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).EtO, steam, e-beam, and gamma sterilizable. Contains mold release.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Density 1.19 g/cc0.0430 lb/in³ISO 1183
Water Absorption 0.14 %0.14 %24 hours; ASTM D570
 0.26 %0.26 %23°C/sat; ISO 62
Moisture Absorption 0.100 %0.100 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inSABIC method
 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
Melt Flow  10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
10 g/10 min
@Load 2.65 lb,
Temperature 572 °F
cm³/10 min; ISO 1133
 10.5 g/10 min
@Load 1.20 kg,
Temperature 300 °C
10.5 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 73.0 MPa10600 psi50 mm/min; ISO 527
 74.0 MPa10700 psi50 mm/min; ASTM D638
Tensile Strength, Yield 61.0 MPa8850 psi50 mm/min; ISO 527
 62.0 MPa8990 psi50 mm/min; ASTM D638
Elongation at Break 128 %128 %50 mm/min; ISO 527
 140 %140 %50 mm/min; ASTM D638
Elongation at Yield 6.0 %6.0 %50 mm/min; ISO 527
 6.5 %6.5 %50 mm/min; ASTM D638
Tensile Modulus 2.30 GPa334 ksi50 mm/min; ASTM D638
 2.39 GPa347 ksi1mm/min; ISO 527
Flexural Yield Strength 93.0 MPa13500 psi2 mm/min; ISO 178
 100 MPa14500 psi1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.25 GPa326 ksi2 mm/min; ISO 178
 2.40 GPa348 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 8.40 J/cm15.7 ft-lb/inASTM D256
 2.20 J/cm
@Temperature -30.0 °C
4.12 ft-lb/in
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 70.0 kJ/m²33.3 ft-lb/in²80*10*3; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NBNB80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
80*10*3; ISO 180/1U
Charpy Impact Unnotched NBNBEdgew 80*10*3 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 7.00 J/cm²33.3 ft-lb/in²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 8.20 J/cm²39.0 ft-lb/in²ISO 179/2C
 1.50 J/cm²
@Temperature -30.0 °C
7.14 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 88.0 J64.9 ft-lbASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  78.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
43.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 78.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
43.3 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow  76.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
42.2 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 76.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
42.2 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Hot Ball Pressure Test 125 °C257 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
@Thickness 6.40 mm
280 °F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 127 °C261 °F1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
 126 °C
@Thickness 3.20 mm
259 °F
@Thickness 0.126 in
unannealed; ASTM D648
 132 °C
@Thickness 6.40 mm
270 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 143 °C289 °FRate B/50; ISO 306
 143 °C289 °FRate B/50; ASTM D1525
 145 °C293 °FRate B/120; ISO 306
 
Processing PropertiesMetricEnglishComments
Processing Temperature 60.0 - 80.0 °C140 - 176 °FHopper Temperature
Nozzle Temperature 270 - 290 °C518 - 554 °FInjection Molding
Zone 1 260 - 280 °C500 - 536 °F
Zone 2 270 - 290 °C518 - 554 °F
Zone 3 280 - 310 °C536 - 590 °F
Melt Temperature 280 - 310 °C536 - 590 °F
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %0.020 %
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10690 / 244157

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.