MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Vitreous Carbon (Glassy Carbon)
Categories: Carbon

Material Notes: Vitreous carbon is formed by the pyrolysis of a carbon-based polymer, such as phenol-formaldehyde, cellulose, or acrylonitrile, under a slow heating scheme. It is a polycrystalline structure with fine grains. The properties, including density, vary depending on the deposition conditions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 - 1.50 g/cc0.0524 - 0.0542 lb/inĀ³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 70.0 - 200 MPa10200 - 29000 psi
Modulus of Elasticity 24.0 - 28.0 GPa3480 - 4060 ksi
Flexural Strength 150 - 200 MPa21800 - 29000 psi
Compressive Strength 700 MPa102000 psi

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Graphite, Carbon, C
Pyrolytic Graphite, Low Temperature Isotropic (LTI)
MarkeTech Carbon Aerogel
Momentive Performance Materials Pyrolytic Graphite (PG) Coating
Diamond, thin film

BGRAP3 / 174

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.