MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Americas Styrenics PolyRenew® 5102 HE High Heat Crystal Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Heat Resistant Grade

Material Notes: Product Characteristics
  • High Efficiency - Fast cycle time
  • High Vicat softening temperature
  • Excellent clarity
  • Food Contact Compliant

Typical Applications

  • Cutlery and Dinnerware
  • Consumer containers, vials, jars, etc.
  • Desk organizers
  • Medical parts

Information provided by AmericasStyrenics LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm0.0040 - 0.0080 in/inASTM D955
Melt Flow 4.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
4.5 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 108108ASTM D785
Tensile Strength at Break 51.0 MPa7400 psiASTM D638
Tensile Strength 51.0 MPa7400 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Tensile Modulus 3.10 GPa450 ksiASTM D638
Flexural Strength 82.7 MPa12000 psiASTM D790
Flexural Modulus 3.28 GPa475 ksiASTM D790
Izod Impact, Notched 0.214 J/cm0.400 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C50.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 95.6 °C204 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 86.7 °C188 °FASTM D648
Vicat Softening Point 104 °C219 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Processing Temperature 66.0 - 104 °C151 - 219 °FPolish Rolls, Extrusion
 204 - 221 °C399 - 430 °FZone 6, Extrusion
 193 - 232 °C379 - 450 °FMelt Pump, Adapter, Pipes, Screen Changer, Extrusion
Nozzle Temperature 230 - 245 °C446 - 473 °FInjection
Zone 1 177 - 193 °C351 - 379 °FExtrusion
 230 - 245 °C446 - 473 °FInjection
Zone 2 182 - 204 °C360 - 399 °FExtrusion
 215 - 230 °C419 - 446 °FInjection
Zone 3 188 - 210 °C370 - 410 °FExtrusion
 200 - 215 °C392 - 419 °FInjection
Zone 4 199 - 216 °C390 - 421 °FExtrusion
Zone 5 204 - 221 °C399 - 430 °FExtrusion
Die Temperature 199 - 232 °C390 - 450 °FExtrusion
Melt Temperature 193 - 232 °C379 - 450 °FExtrusion
Back Pressure 0.172 - 1.48 MPa25.0 - 215 psiInjection
 
Descriptive Properties
Head Pressure10-21 MPaExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAMERI905c / 249347

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.