MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Glyptal CE387 Epoxy Enamel
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: GLYPTAL CE-387 BLUE CATALYST CURING EPOXY is an air-dry epoxy enamel designed to give maximum durability and a high degree of chemical resistance. Because of the durability and chemical resistance, this product is well suited for use as a machinery enamel where resistance to oil, coolants, and other corrosive agents is essential. CE-387 provides excellent adhesion to cleaned steel surfaces. CE-387 is ideally suited for all interior surfaces where maximum durability is required. Often used on windings.

SUGGESTED USES

GLYPTAL CE-387 is designed for use on heavy machinery, industrial equipment, interior walls, metal partitions, and laboratory areas.

APPLICATION

This epoxy enamel is a two-component system consisting of a catalyst and paint. Mix only the amount necessary for immediate use at a ratio of 1 part catalyst by volume to 3 parts paint by volume. Thoroughly mix before using. The pot life of the mixed material is 6-8 hours. GLYPTAL CE387 will not cure without the GLYPTAL 74010 catalyst.

This material may be applied by brush or spray. If necessary, thin mix material with ketones to desired consistency, not to exceed one pint per one gallon of mixed materials. Allow overnight drying between coats. This material should be constantly agitated during use. Surfaces to be painted should be clean and dry.

SURFACE PREPARATION

Surfaces to be painted should be dry and free from dirt, wax, grease, rust, and oil. Remove grease and oil by washing surface with mineral spirits. Allow surface to dry thoroughly. When painting over a glossy surface, reduce gloss by using fine sand paper or steel wool.

Information provided by Glyptal Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 53 %53 %Weight
 
Thermal PropertiesMetricEnglishComments
Flash Point <= 26.7 °C<= 80.0 °F
 
Optical PropertiesMetricEnglishComments
Gloss >= 80 %>= 80 %
 
Processing PropertiesMetricEnglishComments
Dry Time 12.0 hour12.0 hourAir Dry: Touch
Pot Life 4.00 - 6.00 min4.00 - 6.00 minApproximate
 
Descriptive Properties
ColorBlue
Coverage514 ft²/galApproximate; 1 mil dried film
RecoatOvernight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGLYPT928 / 209767

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.