MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M Nextel™ 312 Industrial Ceramic Fiber
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide; Other Engineering Material; Composite Fibers

Material Notes: Chemical composition above is wt%. Crystal phase is mullite + amorphous (or 100% amorphous). Filament diameter is 10-12 µm.

3M Nextel fibers 312, 440, and 550 are designed for non-structural applications where their primary purpose is to act as a flame barrier. 3M Nextel Ceramic Fiber 312 is made from Al2O3, SiO2, and B2O3. Because B2O3 is present, this composition has both crystalline and glassy phases. The glassy phase helps the fiber retain strength after exposure to high temperatures because it slows the growth of crystalline phases that weaken the fiber. However, when the fiber is stressed at high temperature, the glassy phase weakens the fiber due to viscous flow much like a glass fiber.

Information provided by 3M Ceramic Textile and Composites.

Key Words: Alumina, Aluminum Oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.70 g/cc0.0975 lb/in³
Particle Size <= 0.50 µm<= 0.50 µmCrystal size
Specific Surface Area <= 0.20 m²/g<= 0.20 m²/g
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1700 MPa
@Thickness 25.4 mm
247000 psi
@Thickness 1.00 in
filament
Tensile Modulus 150 GPa21800 ksiFilament property
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 5.2
@Frequency 9.375e+9 Hz
5.2
@Frequency 9.375e+9 Hz
Dissipation Factor 0.018
@Frequency 9.375e+9 Hz
0.018
@Frequency 9.375e+9 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 3.00 µm/m-°C
@Temperature 25.0 - 500 °C
1.67 µin/in-°F
@Temperature 77.0 - 932 °F
Specific Heat Capacity 1.05 J/g-°C
@Temperature 500 °C
0.251 BTU/lb-°F
@Temperature 932 °F
Melting Point 1800 °C3270 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5681.568
 
Component Elements PropertiesMetricEnglishComments
Al2O3 62.5 %62.5 %
B2O3 13 %13 %
SiO2 24.5 %24.5 %
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Nextel™ 550 Industrial Ceramic Fiber
3M Nextel™ 440 Industrial Ceramic Fiber
3M Nextel™ 610 Composite Ceramic Fiber
3M Nextel™ 720 Composite Ceramic Fiber
DuPont™ Kevlar® 149 Aramid Fiber, diam. 12 µm

CMMM00 / 1612

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.