FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Hydrolysis resistant; FDA 21 CFR 177.2600 Compliant APPLICATIONS: Solution for soft touch overmolding on consumer electronics, mobile communication devices, computers, and sport &leisure applications; Seals and enclosures.Information provided by Multibase. Multibase is now a DuPont brand; this grade was discontinued prior to DuPont's acquisition. |