MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Extruded

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.01 - 1.20 g/cc0.0365 - 0.0434 lb/in³Average value: 1.07 g/cc Grade Count:195
Water Absorption 0.0500 - 1.00 %0.0500 - 1.00 %Average value: 0.410 % Grade Count:30
Moisture Absorption at Equilibrium 0.000 - 0.300 %0.000 - 0.300 %Average value: 0.217 % Grade Count:13
Water Absorption at Saturation 0.300 - 1.03 %0.300 - 1.03 %Average value: 0.713 % Grade Count:5
Maximum Moisture Content 0.0100 - 0.1500.0100 - 0.150Average value: 0.0476 Grade Count:21
Linear Mold Shrinkage 0.00200 - 0.00800 cm/cm0.00200 - 0.00800 in/inAverage value: 0.00552 cm/cm Grade Count:150
Linear Mold Shrinkage, Transverse 0.00300 - 0.00800 cm/cm0.00300 - 0.00800 in/inAverage value: 0.00575 cm/cm Grade Count:10
Melt Flow 0.100 - 35.0 g/10 min0.100 - 35.0 g/10 minAverage value: 6.37 g/10 min Grade Count:198
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 68.0 - 11868.0 - 118Average value: 106 Grade Count:114
Ball Indentation Hardness 65.0 - 110 MPa9430 - 16000 psiAverage value: 93.2 MPa Grade Count:11
Tensile Strength, Ultimate 22.1 - 74.0 MPa3210 - 10700 psiAverage value: 38.6 MPa Grade Count:60
Tensile Strength, Yield 13.0 - 65.0 MPa1890 - 9430 psiAverage value: 44.7 MPa Grade Count:173
 22.1 - 59.3 MPa
@Temperature -18.0 - 71.0 °C
3210 - 8600 psi
@Temperature -0.400 - 160 °F
Average value: 40.7 MPa Grade Count:1
Elongation at Break 3.00 - 150 %3.00 - 150 %Average value: 48.4 % Grade Count:136
Elongation at Yield 2.00 - 30.0 %2.00 - 30.0 %Average value: 5.44 % Grade Count:57
Modulus of Elasticity 1.00 - 2.65 GPa145 - 384 ksiAverage value: 2.04 GPa Grade Count:64
 1.50 - 2.60 GPa
@Temperature -18.0 - 71.0 °C
218 - 377 ksi
@Temperature -0.400 - 160 °F
Average value: 2.05 GPa Grade Count:1
Flexural Yield Strength 0.379 - 593 MPa55.0 - 86000 psiAverage value: 72.7 MPa Grade Count:149
 49.6 - 113.8 MPa
@Temperature -40.0 - 71.0 °C
7190 - 16510 psi
@Temperature -40.0 - 160 °F
Average value: 81.7 MPa Grade Count:1
Flexural Modulus 0.200 - 5.50 GPa29.0 - 798 ksiAverage value: 2.16 GPa Grade Count:180
 1.90 - 2.80 GPa
@Temperature -40.0 - 71.0 °C
276 - 406 ksi
@Temperature -40.0 - 160 °F
Average value: 2.35 GPa Grade Count:1
Izod Impact, Notched 0.380 - 10.3 J/cm0.712 - 19.3 ft-lb/inAverage value: 4.06 J/cm Grade Count:141
 0.450 - 4.00425 J/cm
@Temperature -40.0 - 0.000 °C
0.843 - 7.50160 ft-lb/in
@Temperature -40.0 - 32.0 °F
Average value: 1.29 J/cm Grade Count:20
 0.200056 - 2.77628 J/cm
@Temperature -40.0 - 0.000 °C
0.374786 - 5.20111 ft-lb/in
@Temperature -40.0 - 32.0 °F
Average value: 1.29 J/cm Grade Count:13
 0.200056 - 2.77628 J/cm
@Thickness 3.17 - 6.40 mm
0.374786 - 5.20111 ft-lb/in
@Thickness 0.125 - 0.252 in
Average value: 1.29 J/cm Grade Count:13
Izod Impact, Unnotched  1.07873 - 1.66713 J/cm
@Temperature -20.0 - -20.0 °C
2.02091 - 3.12322 ft-lb/in
@Temperature -4.00 - -4.00 °F
Average value: 1.37 J/cm Grade Count:2
 1.07873 - 1.66713 J/cm
@Thickness 3.20 - 6.40 mm
2.02091 - 3.12322 ft-lb/in
@Thickness 0.126 - 0.252 in
Average value: 1.37 J/cm Grade Count:2
Izod Impact, Notched (ISO) 8.00 - 48.0 kJ/m²3.81 - 22.8 ft-lb/in²Average value: 26.9 kJ/m² Grade Count:38
 7.00 - 22.0 kJ/m²
@Temperature -30.0 - -20.0 °C
3.33 - 10.5 ft-lb/in²
@Temperature -22.0 - -4.00 °F
Average value: 12.8 kJ/m² Grade Count:16
 7.00 - 21.0 kJ/m²
@Temperature -40.0 - -30.0 °C
3.33 - 9.99 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 12.8 kJ/m² Grade Count:4
 7.00 - 21.0 kJ/m²
@Thickness 4.00 - 4.00 mm
3.33 - 9.99 ft-lb/in²
@Thickness 0.157 - 0.157 in
Average value: 12.8 kJ/m² Grade Count:4
Charpy Impact Unnotched 11.0 J/cm² - NB52.4 ft-lb/in² - NBAverage value: 15.4 J/cm² Grade Count:25
 1.00 J/cm² - NB
@Temperature -40.0 - -30.0 °C
4.76 ft-lb/in² - NB
@Temperature -40.0 - -22.0 °F
Average value: 8.56 J/cm² Grade Count:25
Charpy Impact, Notched 0.700 - 5.00 J/cm²3.33 - 23.8 ft-lb/in²Average value: 2.52 J/cm² Grade Count:52
 0.500 - 2.50 J/cm²
@Temperature -30.0 - -20.0 °C
2.38 - 11.9 ft-lb/in²
@Temperature -22.0 - -4.00 °F
Average value: 1.54 J/cm² Grade Count:21
Dart Drop, Total Energy 24.4 - 50.2 J18.0 - 37.0 ft-lbAverage value: 32.0 J Grade Count:6
Falling Dart Impact 19.0 - 569 J14.0 - 420 ft-lbAverage value: 163 J Grade Count:4
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+9 - 1.00e+17 ohm-cm1.00e+9 - 1.00e+17 ohm-cmAverage value: 7.26e+15 ohm-cm Grade Count:41
Surface Resistance 1.00e+8 - 1.00e+16 ohm1.00e+8 - 1.00e+16 ohmAverage value: 1.24e+15 ohm Grade Count:43
Dielectric Constant 2.60 - 3.302.60 - 3.30Average value: 2.99 Grade Count:19
Dielectric Strength 18.0 - 50.0 kV/mm457 - 1270 kV/inAverage value: 33.0 kV/mm Grade Count:24
Dissipation Factor 0.00500 - 0.09000.00500 - 0.0900Average value: 0.0222 Grade Count:18
Comparative Tracking Index 525 - 600 V525 - 600 VAverage value: 590 V Grade Count:18
Hot Wire Ignition, HWI 7.00 - 60.0 sec7.00 - 60.0 secAverage value: 19.7 sec Grade Count:6
High Amp Arc Ignition, HAI 120 - 200 arcs120 - 200 arcsAverage value: 160 arcs Grade Count:6
High Voltage Arc-Tracking Rate, HVTR 0.000 - 25.4 mm/min0.000 - 1.00 in/minAverage value: 5.90 mm/min Grade Count:6
 
Thermal PropertiesMetricEnglishComments
CTE, linear 40.0 - 110 µm/m-°C22.2 - 61.1 µin/in-°FAverage value: 82.8 µm/m-°C Grade Count:70
CTE, linear, Transverse to Flow 87.0 - 104 µm/m-°C48.3 - 58.0 µin/in-°FAverage value: 97.9 µm/m-°C Grade Count:5
Thermal Conductivity 0.150 - 0.200 W/m-K1.04 - 1.39 BTU-in/hr-ft²-°FAverage value: 0.171 W/m-K Grade Count:11
Maximum Service Temperature, Air 80.0 - 100 °C176 - 212 °FAverage value: 89.2 °C Grade Count:4
Deflection Temperature at 0.46 MPa (66 psi) 70.0 - 107 °C158 - 225 °FAverage value: 94.6 °C Grade Count:55
Deflection Temperature at 1.8 MPa (264 psi) 70.0 - 130 °C158 - 266 °FAverage value: 95.8 °C Grade Count:172
Vicat Softening Point 87.0 - 125 °C189 - 257 °FAverage value: 99.9 °C Grade Count:135
Glass Transition Temp, Tg 108 - 109 °C226 - 228 °FAverage value: 108 °C Grade Count:3
UL RTI, Electrical 50.0 - 120 °C122 - 248 °FAverage value: 85.0 °C Grade Count:47
UL RTI, Mechanical with Impact 50.0 - 105 °C122 - 221 °FAverage value: 83.1 °C Grade Count:42
UL RTI, Mechanical without Impact 50.0 - 120 °C122 - 248 °FAverage value: 88.0 °C Grade Count:41
Flammability, UL94 HB - V-0HB - V-0Grade Count:148
Oxygen Index 19.0 %19.0 %Average value: 19.0 % Grade Count:7
Glow Wire Test 650 - 960 °C1200 - 1760 °FAverage value: 677 °C Grade Count:20
 
Optical PropertiesMetricEnglishComments
Gloss 2.50 - 98.0 %2.50 - 98.0 %Average value: 69.3 % Grade Count:20
Transmission, Visible 0.000 - 91.0 %0.000 - 91.0 %Average value: 70.5 % Grade Count:37
 
Processing PropertiesMetricEnglishComments
Processing Temperature 76.7 - 240 °C170 - 464 °FAverage value: 169 °C Grade Count:12
Nozzle Temperature 180 - 310 °C356 - 590 °FAverage value: 273 °C Grade Count:46
Adapter Temperature 200 - 300 °C392 - 572 °FAverage value: 273 °C Grade Count:43
Die Temperature 200 - 295 °C392 - 563 °FAverage value: 263 °C Grade Count:44
Melt Temperature 170 - 320 °C338 - 608 °FAverage value: 260 °C Grade Count:99
Mold Temperature 29.0 - 120 °C84.2 - 248 °FAverage value: 74.0 °C Grade Count:82
Injection Velocity 240 mm/sec9.45 in/secAverage value: 240 mm/sec Grade Count:8
Roll Temperature 60.0 - 150 °C140 - 302 °FAverage value: 121 °C Grade Count:43
Drying Temperature 70.0 - 120 °C158 - 248 °FAverage value: 90.2 °C Grade Count:108
Moisture Content 0.0100 - 0.0300 %0.0100 - 0.0300 %Average value: 0.0197 % Grade Count:37
Injection Pressure 4.83 - 150 MPa700 - 21800 psiAverage value: 35.7 MPa Grade Count:15

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Overview of materials for Polycarbonate, Extruded
ALM PA 650 Nylon 12 SLS Prototyping Polymer
Overview of materials for Polylactic Acid (PLA) Biopolymer
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

O1106 / 77797

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.