MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bakelite® UP 3415 Unsaturated Polyester Resin, Low Shrinkage, High Arc Resistance, UL Listed, High Mechanical Strength
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: Polyester molding compound, inorganically filled, glass fiber reinforced, styrene free, very high dimensional stability, non flammable, high mechanical properties, UL listed molding compound 0.75 mm / V-0 (ALL), RTI 170 °C.

Applications: Safety switch housings and electrotechnical parts, e. g. energy regulators, clamp boards, lamp parts, MCB housings, MCCB housings, excellent RTI of 170°C

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.00 g/cc0.0723 lb/in³ISO 1183
Apparent Bulk Density 0.900 g/cc0.0325 lb/in³ISO 60
Linear Mold Shrinkage 0.0015 cm/cm0.0015 in/inCompression Molding. Post Shrinkage = 0.02%.; ISO 2577
 0.0030 cm/cm0.0030 in/inInjection Molding. Post Shrinkage = 0.02%.; ISO 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 325 MPa47100 psiH961/30; ISO 2039/P1
Tensile Strength 45.0 MPa6530 psiISO 527 - 1/2
Tensile Modulus 10.0 GPa1450 ksiISO 527 - 1/2
Flexural Strength 105 MPa15200 psiISO 178
Flexural Modulus 13.0 GPa1890 ksiISO 178
Compressive Strength 160 MPa23200 psiISO 604
Charpy Impact Unnotched 0.850 J/cm²4.04 ft-lb/in²ISO 179-1 eU
Charpy Impact, Notched 0.450 J/cm²2.14 ft-lb/in²ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cm
Surface Resistance 1.00e+12 ohm1.00e+12 ohm
Dielectric Constant 5.25
@Frequency 100 Hz
5.25
@Frequency 100 Hz
Dielectric Strength 25.0 kV/mm
@Thickness 1.00 mm
635 kV/in
@Thickness 0.0394 in
IEC 60243-P1
Dissipation Factor 0.020
@Frequency 100 Hz
0.020
@Frequency 100 Hz
Arc Resistance 190 - 195 sec190 - 195 secASTM D495
High Voltage Arc Resistance to Ignition (HVAR) >= 300 sec
@Thickness 0.750 mm
>= 300 sec
@Thickness 0.0295 in
ALL
Comparative Tracking Index 600 V600 V
Hot Wire Ignition, HWI  60 - 120 sec
@Thickness 0.750 mm
60 - 120 sec
@Thickness 0.0295 in
ALL
 >= 120 sec
@Thickness 1.50 mm
>= 120 sec
@Thickness 0.0591 in
ALL
High Amp Arc Ignition, HAI  30 - 60 arcs
@Thickness 0.750 mm
30 - 60 arcs
@Thickness 0.0295 in
ALL
 60 - 120 arcs
@Thickness 1.50 mm
60 - 120 arcs
@Thickness 0.0591 in
ALL
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
@Thickness 3.00 mm
0.000 - 0.394 in/min
@Thickness 0.118 in
(ALL)
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 180 °C356 °F<20000 hours; IEC 60216-P1
 200 °C392 °F< 50 hours; IEC 60216-P1
Deflection Temperature at 8.0 MPa 210 °C410 °FISO 75-2
UL RTI, Electrical 170 °C
@Thickness 0.750 mm
338 °F
@Thickness 0.0295 in
ALL
UL RTI, Mechanical with Impact  130 °C
@Thickness 0.750 mm
266 °F
@Thickness 0.0295 in
ALL
 170 °C
@Thickness 3.00 mm
338 °F
@Thickness 0.118 in
(ALL)
UL RTI, Mechanical without Impact  130 °C
@Thickness 0.750 mm
266 °F
@Thickness 0.0295 in
ALL
 170 °C
@Thickness 3.00 mm
338 °F
@Thickness 0.118 in
(ALL)
Flammability, UL94 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
All colors
 
Processing PropertiesMetricEnglishComments
Feed Temperature 60.0 - 70.0 °C140 - 158 °FInjection molding
Nozzle Temperature 70.0 - 100 °C158 - 212 °FInjection molding
Melt Temperature 70.0 - 100 °C158 - 212 °FInjection molding
Mold Temperature 160 - 180 °C320 - 356 °FInjection molding
 160 - 180 °C320 - 356 °FCompression molding
Injection Pressure >= 10.0 MPa>= 1450 psiCompression and injection cavity mold pressure
Back Pressure 0.500 - 1.00 MPa72.5 - 145 psiInjection molding
Cure Time 0.167 - 0.333 min0.00278 - 0.00556 hourPer 1 mm of wall thickness, injection molding
 0.333 - 0.667 min0.00556 - 0.0111 hourPer 1 mm of wall thickness, compression molding
 
Descriptive Properties
Creep Rupture StrengthGood
Holding PressureApproximately 40-60% of injection pressure
Media ResistanceMedium
Thermal ExpansionVery Slight
Water absorption (mg)2024h / 23°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bakelite® UP 804 Unsaturated Polyester Resin, High Surface Quality, UL Listed, Low Shrinkage, High Arc Resistance
Bakelite® UP 3620 Unsaturated Polyester Resin, High Surface Quality, UL Listed
Bakelite® UP 802 Unsaturated Polyester Resin, High Surface Quality, Low Shrinkage, High Arc Resistance
Bakelite® UP 3420 Unsaturated Polyester Resin, High Mechanical Strength, High Arc Resistance, UL Listed, Low Shrinkage
Menzolit Menzolit® BMC 0160 Unsaturated Polyester UP

PBAKE053 / 27087

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.