MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AdvanSix Aegis® HCA95MP Nylon 6/6,6 Extrusion Grade Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, Unreinforced

Material Notes: Description: Aegis HCA95MP is a low viscosity nylon 6/6,6 copolymer extrusion grade. It conforms to Food and Drug Administration requirements of 21 CFR177.1500. Aegis HCA73ZP possesses the combination of strength and toughness associated with nylon 6/6,6 as well as excellent heat, chemical, and abrasion resistance. The reduced melt point (385 degF/196 degC) of this resin results in lower process melt temperature, lower head pressure, and lower amperage. This translates to higher extrusion rates and thinner nylon layer capabilities. It will also thermoform at lower temperatures and yield higher production rates.

Applications:

  • Processed Meat
  • Fresh Red Meat
  • Poultry
  • Fish
  • Cheese
  • Dried Food
  • Chilled Fruit Juices

Former Honeywell product; AdvanSix is a spin-off of Honeywell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccASTM D1505
Water Absorption 0.80 %0.80 %Extractable Content
 1.4 %1.4 %in 24 hours
Moisture Absorption at Equilibrium 2.5 %2.5 %at 50% RH
Water Absorption at Saturation 9.0 %9.0 %
Oxygen Transmission Rate 37.2 cc/m²/day2.40 cc/100 in²/day
Nitrogen Transmission 7.80 cc-mm/m²-24hr-atm19.8 cc-mil/100 in²-24hr-atmcc/m²/day, No thickness given
Carbon Dioxide Transmission 113 cc-mm/m²-24hr-atm287 cc-mil/100 in²-24hr-atmcc/m²/day, No thickness given
Viscosity Measurement 3.03.096% SAV
 7373FAV; ASTM D789
Maximum Moisture Content 0.0800.080
Melt Flow 4.5 g/10 min
@Load 1.00 kg,
Temperature 235 °C
4.5 g/10 min
@Load 2.20 lb,
Temperature 455 °F
ASTM D1238
 
Thermal PropertiesMetricEnglishComments
Melting Point 200 °C392 °FASTM D3418
 
Processing PropertiesMetricEnglishComments
Middle Barrel Temperature 225 - 245 °C437 - 473 °FTubular (Blown) Film
 225 - 250 °C437 - 482 °FCast Film
Adapter Temperature 243 °C469 °FTubular (Blown) Film
 250 °C482 °FCast Film
Die Temperature 240 °C464 °FCast Film
 240 °C464 °FTubular (Blown) Film
Melt Temperature 243 °C469 °FTubular (Blown) Film
 248 °C478 °FCast Film
Moisture Content 0.080 %0.080 %
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AdvanSix Aegis® HCA73MP Nylon 6/6,6 Extrusion Grade Copolymer
AdvanSix Aegis® HCA73ZP Nylon 6/6,6 Extrusion Grade Copolymer
A. Schulman Lucent 66-01 Nylon 66, General Purpose, Injection Grade
A. Schulman Lucent 6-01 Nylon 6, General Purpose, Injection Grade
AdvanSix Aegis® HCA115QP Nylon 6/6,6 Extrusion Grade Copolymer

PALA26 / 23118

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.