MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Europium, Eu
Categories: Metal; Nonferrous Metal; Pure Element

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 5.26 g/cc0.190 lb/in³
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 151.964151.9641995
Atomic Number 6363
X-ray Absorption Edge 0.25552 Å0.25552 ÅK
 1.53815 Å1.53815 ÅLI
 1.62591 Å1.62591 ÅLII
 1.77491 Å1.77491 ÅLIII
Ionic Radius 0.950 Å0.950 ÅCrystal Ionic Radius for Valence +3
 1.09 Å1.09 ÅCrystal Ionic Radius for Valence +2
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 1717
Tensile Modulus 18.2 GPa2640 ksi
Bulk Modulus 8.30 GPa1200 ksi
Poissons Ratio 0.1520.152
Shear Modulus 7.90 GPa1150 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000910 ohm-cm0.0000910 ohm-cm
Magnetic Susceptibility 0.0002180.000218cgs/g
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 61.0 J/g26.2 BTU/lb
CTE, linear 35.0 µm/m-°C
@Temperature 20.0 °C
19.4 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.160 J/g-°C0.0382 BTU/lb-°F
Thermal Conductivity 13.9 W/m-K96.5 BTU-in/hr-ft²-°F
Melting Point 817 - 827 °C1500 - 1520 °F
Boiling Point 1529 °C2784 °F
 
Component Elements PropertiesMetricEnglishComments
Europium, Eu 100 %100 %
 
Descriptive Properties
CAS Number7440-53-1

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Americium, Am
Silver, Ag
Aluminum, Al
Chromium, Cr; Recrystallized
Copper, Cu; Cold-Worked

AMEEu00 / 34

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.