MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Goodfellow Cellulose Acetate
Categories: Polymer; Film; Thermoplastic; Cellulosic; Cellulose Acetate, Molded

Material Notes: An amorphous, transparent and colorless, glossy and reasonably hard thermoplastic with good clarity but only moderate UV stability and chemical resistance. Its high moisture absorption can lead to the normal difficulties of dimensional changes.

Applications include spectacle frames, tool and brush handles and packaging including stiff thin-walled tubes for "display packaging". Films are widely used for graphics purposes and are available from stock in selected thicknesses (and other thicknesses as special orders).

Brand names include Clarifoil, Dexel, and Tenite Acetate.

Information provided by Goodfellow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³
Water Absorption 1.9 - 7.0 %
@Time 86400 sec
1.9 - 7.0 %
@Time 24.0 hour
Oxygen Transmission 20.5 cc-mm/m²-24hr-atm
@Temperature 25.0 °C
52.0 cc-mil/100 in²-24hr-atm
@Temperature 77.0 °F
Film
Nitrogen Transmission 17.5 cc-mm/m²-24hr-atm
@Temperature 25.0 °C
44.5 cc-mil/100 in²-24hr-atm
@Temperature 77.0 °F
Film
Carbon Dioxide Transmission 1480 cc-mm/m²-24hr-atm
@Temperature 25.0 °C
3760 cc-mil/100 in²-24hr-atm
@Temperature 77.0 °F
Film
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 12.0 - 110 MPa1740 - 16000 psi
Elongation at Break 15 - 55 %15 - 55 %Film
Tensile Modulus 1.00 - 4.00 GPa145 - 580 ksi
Izod Impact, Notched 1.00 - 4.50 J/cm1.87 - 8.43 ft-lb/in
Tear Strength 0.177 - 0.353 kN/m1.01 - 2.02 pliFilm
Taber Abrasion, mg/1000 Cycles 6565
Heat Seal Strength Initiation Temperature 176 - 232 °C349 - 450 °FFilm
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 5.0
@Frequency 1e+6 Hz
5.0
@Frequency 1e+6 Hz
Dielectric Strength 11.0 kV/mm279 kV/in
Dissipation Factor  0.0038
@Frequency 1e+6 Hz
0.0038
@Frequency 1e+6 Hz
Film
 0.060
@Frequency 1000 Hz
0.060
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 - 180 µm/m-°C44.4 - 100 µin/in-°F
Specific Heat Capacity 1.20 - 1.90 J/g-°C0.287 - 0.454 BTU/lb-°F
Thermal Conductivity 0.160 - 0.360 W/m-K1.11 - 2.50 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 55.0 - 95.0 °C131 - 203 °F
Deflection Temperature at 0.46 MPa (66 psi) 52.0 - 105 °C126 - 221 °F
Deflection Temperature at 1.8 MPa (264 psi) 48.0 - 86.0 °C118 - 187 °F
Minimum Service Temperature, Air -20.0 °C-4.00 °F
Flammability, UL94 HBHB
Oxygen Index 19 %19 %
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.491.49
 
Descriptive Properties
Radiation resistanceFair
UV resistanceFair

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOODF247 / 254986

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.