MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik VESTAMID® DX9330 Nylon 612
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Unreinforced

Material Notes: VESTAMID® DX9330 NC is a PA 612 base polymer without any stabilizers and other additives. VESTAMID® DX9330 NC is suitable for both extrusion as well as injection molding. Usually VESTAMID® DX9330 NC is only used in special cases when additives are not preferable, or processing aids are not necessary, e.g. filament extrusion. Based on the perfect balance of amino and carboxyl end groups this material is easy to process and to dye. The typical characteristics of PA 612 are moderate water absorption, good dimensional stability and almost unchanged properties at varying ambient humidity. VESTAMID® DX9330 NC is supplied as cylindrical granules, ready for processing, in moisture-proof bags. The processing temperature should be within a range of 250°C to 290°C. Pigmentation may affect values. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
Dry properties listed below
Industrial Sector: Sustainable, Sports and Lifestyle
Sustainability: Sustainable electricity
Processing: Injection molding
Delivery form: Pellets, Granules
Conformity: Food contact
Additives: Unfilled
Applications: Medium viscosity
Color: Natural color

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ISO 1183
Water Absorption 2.80 %2.80 %Sim to ISO 62
Moisture Absorption 1.40 %1.40 %Sim to ISO 62
Viscosity Number 155 cm³/g1.55 dl/gISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.0140 cm/cm0.0140 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0140 cm/cm0.0140 in/inISO 294-4, 2577
Melt Flow 69.0 g/10 min
@Load 10.0 kg,
Temperature 240 °C
69.0 g/10 min
@Load 22.0 lb,
Temperature 464 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 44.0 MPa6380 psiISO 527
Tensile Strength 58.0 MPa8410 psiISO 527
Tensile Stress 42.0 MPa
@Strain 50.0 %
6090 psi
@Strain 50.0 %
ISO 527
Tensile Strength, Yield 58.0 MPa8410 psiISO 527
Elongation at Break >= 50.0 %>= 50.0 %Nominal; ISO 527
Elongation at Yield 4.00 %4.00 %ISO 527
Tensile Modulus 2.20 GPa319 ksiISO 527
Flexural Strength 69.0 MPa10000 psiat conv. Deflection; ISO 178
 83.0 MPa12000 psiISO 178
Flexural Modulus 2.06 GPa299 ksiISO 178
Flexural Strain at Break 6.00 %6.00 %at flexural strength; ISO 178
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.450 J/cm²
@Temperature 23.0 °C
2.14 ft-lb/in²
@Temperature 73.4 °F
Type of failure: C; ISO 179/1eA
 0.450 J/cm²
@Temperature -30.0 °C
2.14 ft-lb/in²
@Temperature -22.0 °F
Type of failure: C; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 215 °C419 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 149 °C300 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °C136 °FISO 75-1/-2
Vicat Softening Point  180 °C
@Load 5.10 kg
356 °F
@Load 11.2 lb
50 K/h; ISO 306
 211 °C
@Load 1.02 kg
412 °F
@Load 2.25 lb
50 K/h; ISO 306
Glass Transition Temp, Tg 44.0 °C111 °FISO 11357-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 °C482 °FInjection Molding; ISO 294
 250 °C482 °F
Mold Temperature 80.0 °C176 °FInjection Molding; ISO 294
 80.0 °C176 °F
Injection Velocity 200 mm/sec7.87 in/secInjection Molding; ISO 294
Moisture Content 0.150 %0.150 %ISO 15512
 
Descriptive Properties
Blue water consumption10.8 kgISO 14040, 14044
Color-0.01b, CIE
 Natural color
Flexural stress at breakNMPa, ISO 178
 N%, ISO 178
Global Warming Potential1.2 kg CO2 eq./kgsavings incl. bio. C. as compared to classical production, ISO 14040, 14044
 6.9 kg CO2 eq./kgincl. bio. C incl. LUC, ISO 14040, 14044
 6.9 kg CO2 eq./kgexcl. bio. C incl. LUC, ISO 14040, 14044
Land use (ReCiPe 2016)0.1 Annual crop eq. yISO 14040, 14044

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK7896 / 325028

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.