MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SEKISUI SPI ALLEN® 2175HG Medium Impact ABS Sheet
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Sheet

Material Notes: ALLEN® 2175HG is a general purpose ABS with medium impact and a high gloss finish.

ALLEN® 2175HG has been tested under laboratory conditions and has achieved a UL94 HB rating at 0.060 in (1.52mm) and above and meets the requirements of Federal Motor Vehicle Safety Standard No. 302 (FMVSS 302).

Suggested Application:

  • Medical Equipment Housings
  • Food Equipment Trays & Housings
  • Display
  • Signs
Features:
  • Custom color matching
  • Good forming and fabricating properties
  • Edge trim easily used in future orders
  • High gloss finish

Information provided by SEKISUI KYDEX, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/ccASTM D792
Linear Mold Shrinkage 0.000400 - 0.00700 cm/cm0.000400 - 0.00700 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 35.8 MPa5190 psiASTM D638
Flexural Strength 59.2 MPa8590 psiASTM D790
Flexural Modulus 2.00 GPa290 ksiASTM D790
Izod Impact, Notched  1.28 J/cm
@Temperature -18.0 °C
2.40 ft-lb/in
@Temperature -0.400 °F
ASTM D256
 2.61 J/cm
@Temperature 23.0 °C
4.89 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 93.4 °C200 °Fannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 87.8 °C190 °Fannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.52 mm
HB
@Thickness 0.0598 in
 
Optical PropertiesMetricEnglishComments
Gloss 80.0 %80.0 %60° Angle; ASTM D523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSEKIS553 / 325293

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.