MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Materion SupremEX® 620ZF Aluminum - Silicon Carbide Metal Matrix Composite, T1(As Rolled), Rolled Sheet
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Aluminum Alloy

Material Notes: SupremEX 620ZF is a high-quality aerospace-grade aluminum alloy (6063) reinforced with 20 vol.% silicon carbide particles which produces a metal matrix composite (MMC). The MMC is manufactured via a powder metallurgy route using a mechanical alloying process to ensure a homogeneous reinforcement distribution. This provides a refined grain structure, which enhances mechanical properties. SupremEX 620ZF is heat treatable to offer high strength and modulus for structural applications. Designation – 6063/SiC/20p (0.7µm)

Advantages

  • Weight saving
  • Increased component stiffness
  • Strength & fatigue resistance
  • Formability
  • Hardness, wear resistance & low friction characteristics
  • Machinable using conventional high-speed techniques
  • Corrosion performance
  • Homogeneous, stable microstructure

Information provided by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.80 g/cc0.101 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 372 MPa54000 psi
Tensile Strength, Yield 290 MPa
@Strain 0.200 %
42000 psi
@Strain 0.200 %
Elongation at Break 11.0 %11.0 %
Modulus of Elasticity 99.0 GPa14400 ksi
Poissons Ratio 0.3000.300
Shear Modulus 38.0 GPa5510 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000440 - 0.00000450 ohm-cm0.00000440 - 0.00000450 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.9 µm/m-°C9.40 µin/in-°F
Solidus 570 °C1060 °F
 
Descriptive Properties
Specific Stiffness35.7 GPa/g/cm3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NBB9113p / 323551

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.