MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Opti-Polymers Optilox PBT GK20 ST PBT, 20% Glass Pearls Filled
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass Bead Filled

Material Notes: PBT compound with increased stiffness and low warping tendency and low shrinkage. Different colors available.

Information provided by Opti-Polymer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.49 g/cc0.0538 lb/in³ISO 1183
Maximum Moisture Content 0.20
@Temperature 120 °C,
Time 299 sec
0.20
@Temperature 248 °F,
Time 0.0830 hour
thermogravimetric
Melt Flow 25 g/10 min25 g/10 minISO 1133
Ash 18 - 23 %
@Temperature 625 °C
18 - 23 %
@Temperature 1160 °F
ISO 3451
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 45.0 MPa6530 psi5 mm / min; ISO 527-1
Elongation at Break >= 3.0 %
@Time 86400 sec
>= 3.0 %
@Time 24.0 hour
5 mm / min, 50% RH; ISO 527-1
Tensile Modulus 2.75 GPa399 ksi1 mm / min; ISO 527-1
Charpy Impact, Notched 0.260 J/cm²1.24 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 160 °C320 °FISO75-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 °C428 °Finjection molding
Mold Temperature 50.0 - 80.0 °C122 - 176 °Finjection molding
Drying Temperature 105 °C221 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
 
Descriptive Properties
Regional AvailabilityEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

POPTI006 / 255142

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.