MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Koattro PB M 8911M Polybutene Random Copolymer
Categories: Polymer; Thermoplastic; Polybutene

Material Notes: Polybutene-1 grade Koattro PB M 8911M is a random copolymer of butene-1 with high ethylene content. Koattro PB M 8911M is primarily used as a blend component in woodworking and assembly hot melt adhesive formulations. It can be used in combination with a wide variety of non-polar resins and waxes and maintains good cohesive strength of the HMA and higher Shear Adhesion Failure Temperature (SAFT). Koattro PB M 8911M is also used to improve rheological properties in blends. It is highly compatible with polypropylene due to its similar structure. Koattro PB M 8911M is less compatible but still easily dispersible in blends with polyethylene. Its relatively slow kinetics of crystallization allow for an excellent wetting behavior. Its high shear-sensitive flow behavior means that it remains easily dispersible also in even more incompatible polymers like thermoplastic elastomers. Koattro PB M 8911M can also be used in Melt Blown and Spunbond applications offering reduced bonding temperature and improved softness. This grade is not intended for medical and pharmaceutical applications.

Status: Commercial – Active

Availability: Africa-Middle East; Asia-Pacific; Australia and New Zealand; Europe; North America; South & Central America

Application: Hot Melt Adhesives; Hygiene Nonwoven; Polymer Modifier

Market: Compounding; Textile

Processing Method: Extrusion Coating; Melt Blown; Spunbond

Attribute: Extended Open Time; Good Adhesion; Good Thermal Stability

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.895 g/cc0.0323 lb/in³ISO 1183-1
Brookfield Viscosity 46600 cP
@Temperature 190 °C
46600 cP
@Temperature 374 °F
ASTM D3236
Melt Flow 200 g/10 min
@Load 2.16 kg,
Temperature 190 °C
200 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Modulus 0.100 GPa14.5 ksiISO 527-1, -2
 
Thermal PropertiesMetricEnglishComments
Melting Point 82.0 °C180 °FTm2; ISO 11357-3
 93.0 °C199 °FTm1; ISO 11357-3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9642 / 324577

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.