MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hapco ULTRALLOY 207 Polyurethane Liquid
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Liquid

Material Notes: A series of general purpose Liquid Molding Compounds that do not change color and remain clear/light yellow when cured. Ultralloy 200 Series are ideal for in mold coloring of parts. They can be easily pigmented and the color remains the same in the cured or liquid state. Tensile strengths from 10,300 psi to 11,800 psi are available:
  • 1:1 by weight
  • Available in 2 speeds
  • Clear/translucent when cured

Information provided by Hapco, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccASTM D-4669
Viscosity 225 - 325 cP225 - 325 cPASTM D-4878
Linear Mold Shrinkage 0.0010 - 0.0040 cm/cm0.0010 - 0.0040 in/inASTM D-2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8686ASTM D-2240
Tensile Strength 81.4 MPa11800 psiASTM D-638
Elongation at Break 8.3 %8.3 %ASTM D-638
Modulus of Elasticity 1.77 GPa256 ksiASTM D-638
Flexural Strength 82.0 MPa11900 psiASTM D-790
Flexural Modulus 2.21 GPa320 ksiASTM D-790
Izod Impact, Notched 0.416 J/cm0.780 ft-lb/inASTM D-256
Izod Impact, Unnotched >= 3.43 J/cm>= 6.42 ft-lb/inASTM D-256
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature 73.0 °C163 °FASTM D-648
 
Processing PropertiesMetricEnglishComments
Cure Time 45.0 - 90.0 min
@Thickness 3.17 mm
0.750 - 1.50 hour
@Thickness 0.125 in
Demold
Gel Time 8.50 min
@Load 0.100 kg
8.50 min
@Load 0.221 lb
ASTM D-2971
 
Descriptive Properties
Color (cured)clear / slight yellow
Mix Ratio100:100Weight
 100:115Volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHAPCO185 / 317244

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.