MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Momentive Performance Materials HCR48 Boron Nitride (BN) Powder
Categories: Ceramic; Nitride; Other Engineering Material; Additive/Filler for Polymer

Material Notes: GE Advanced Ceramics boron nitride (BN) powder grades HCR48, HCJ48, and HCM are large, high-density agglomerates, of ~10 µm crystals, with average particle sizes between 175-275 µm and tap densities of ~1 g/cm3. These features, combined with low average surface areas, give powders that flow readily, withstand harsh processing, and have outstanding thermal characteristics.

HCR48 has an average particle size of 250 µm and is the highest density (hardest) grade offered by GE Advanced Ceramics. It has higher oxygen and soluble borate levels than most grades, which limits its performance in high-temperature (>550o C) applications.

Information provided by Momentive Performance Materials, formerly GE Advanced Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 1.10 g/cc0.0397 lb/in³Tap Density
Particle Size 10 µm10 µmCrystal Size
 250 µm250 µmMean
Specific Surface Area 2.6 m²/g2.6 m²/g
 
Descriptive Properties
Carbon0.2%
ColorWhite
Crystal TypeHexagonal (Graphitic)
Oxygen2.5%
Sol. Borate3%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cadmium, Cd
Momentive Performance Materials HCPH Boron Nitride (BN) Powder
Momentive Performance Materials PolarTherm® PT140 Boron Nitride (BN) Powder
Tellurium, Te
Titanium Nitride (TiN) Coating

CADV23 / 415

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.