MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Mid-Mountain Materials CERMEX® MT1200 Thermal Insulation Mat
Categories: Ceramic; Glass; Glass Fiber; Other Engineering Material; Composite Fibers

Material Notes: CERMEX® MT1200 is a non-woven insulation mat for use in high temperature applications up to 1600°F (871°C). The fibers are mechanically bonded and contain no additional resins or adhesives. The structure of the material allows for conformability to irregular surfaces and is easily cut and fabricated to intricate configurations. Typical applications include thermal insulations, engine exhaust systems, engine heat component heat shields, industrials furnaces, and turbine insulation. Material: Mineral Fiber, Construction: Needled Blanket

Information provided by Mid-Mountain Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0961 g/cc0.00347 lb/in³
 0.144 g/cc0.00521 lb/in³
 0.192 g/cc0.00694 lb/in³
Filament Diameter 9.0 µm9.0 µm
Thickness 6350 microns250 mil
 12700 microns500 mil
 19050 microns750.0 mil
 25400 microns1000 mil
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0720 W/m-K
@Temperature 260 °C
0.500 BTU-in/hr-ft²-°F
@Temperature 500 °F
 0.154 W/m-K
@Temperature 538 °C
1.07 BTU-in/hr-ft²-°F
@Temperature 1000 °F
 0.205 W/m-K
@Temperature 649 °C
1.42 BTU-in/hr-ft²-°F
@Temperature 1200 °F
 0.336 W/m-K
@Temperature 871 °C
2.33 BTU-in/hr-ft²-°F
@Temperature 1600 °F
Maximum Service Temperature, Air 871 °C1600 °FContinuous
Shrinkage <= 5.0 %
@Temperature 816 °C
<= 5.0 %
@Temperature 1500 °F
 
Descriptive Properties
Roll Length (ft)Various
Shot Content (%)None
Width (in)40
 60

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mid-Mountain Materials PADMAT® MT1000 Needled Fiberglass Mat
Thermal Ceramics Kaomat SL Blanket
Thermal Ceramics Kaomat Blanket
Rogers Arlon 920-20Bxx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape

CMID64 / 141232

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.