MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik VESTOPLAST® 308 Amorphous Polyalphaolefin
Categories: Polymer; Thermoplastic; Polyalphaolefin

Material Notes: VESTOPLAST 308 is a functionalized, amorphous polyalphaolefin, and butene-rich. Generally used as hot melt adhesives with good adhesion to metal and polar substrates.

Key Words: APAO
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.870 g/cc
@Temperature 23.0 °C
0.0314 lb/in³
@Temperature 73.4 °F
Viscosity 6000 - 10000 cP
@Temperature 190 °C
6000 - 10000 cP
@Temperature 374 °F
melt, rotational viscometer; DIN 53 019
Molecular Weight 11300 g/mol11300 g/molMn; GPC
 49000 g/mol49000 g/molMw; GPC
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 1.50 MPa218 psiDIN EN ISO 527-3
Elongation at Break 500 %500 %DIN EN ISO 527-3
Shear Modulus 0.0140 GPa
@Temperature 23.0 °C
2.03 ksi
@Temperature 73.4 °F
DIN EN ISO 6721-2
Penetration 14 - 20
@Thickness 0.100 mm
14 - 20
@Thickness 0.00394 in
needle 100/25/5; DIN 52 010
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 65.0 - 70.0 °C149 - 158 °Funder load 5 °C/h, weight 450g; Degussa Method
Glass Transition Temp, Tg -29.0 °C-20.2 °FDSC
Ring & Ball Softening Point 130 - 142 °C266 - 288 °FDIN 52 011
 
Descriptive Properties
Open Time (sec)240Degussa Method
Setting Time (sec)1Degussa Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik VESTOPLAST® 206 + 6%, 206 B Amorphous Polyalphaolefin
Evonik VESTOPLAST® EP NC 702 Amorphous Polyalphaolefin
Overview of materials for Polyalphaolefin
Evonik VESTOPLAST® 750 Amorphous Polyalphaolefin
Evonik VESTOPLAST® 708 Amorphous Polyalphaolefin

PHUMB412 / 81414

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.