MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECASON P MT XRO® red Polyphenylsulfone, barium sulfate filled
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes:
  • x-ray opaque
  • high thermal and mechanical capacity
  • good heat deflection temperature
  • hydrolysis and superheated steam resistant
  • good impact strength
  • high gamma radiation resistance
  • good chemical resistance
  • high strength
Target Industries:
  • medical technology

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³
Moisture Absorption 0.190 %
@Time 86400 sec
0.190 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9292ASTM D785
Hardness, Rockwell R 126126ASTM D785
Tensile Strength, Yield 79.3 MPa11500 psiASTM D638
Elongation at Break 35 %35 %ASTM D638
Modulus of Elasticity 2.90 GPa420 ksiASTM D638
Flexural Strength 124 MPa18000 psiASTM D790
Flexural Modulus 2.41 GPa350 ksiASTM D790
Compressive Yield Strength 94.5 MPa
@Strain 10 %
13700 psi
@Strain 10 %
ASTM D695
Compressive Strength 12.1 MPa
@Strain 1 %
1750 psi
@Strain 1 %
ASTM D695
Compressive Modulus 1.55 GPa225 ksiASTM D695
Izod Impact, Notched 0.854 J/cm1.60 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °FLong Term
 
Descriptive Properties
Colorred

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN8218 / 319146

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.