MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips 66 HD Calcium Grease NLGI No. 1
Categories: Fluid; Lubricant; Calcium Gellant; Organic Soap Gellant

Material Notes: Description: Conoco HD Calcium Grease is a formulated product, ideally suited for equipment exposed to corrosive fluids, saltwater or extremely high temperatures. HD Calcium Grease is used exclusively by NASA in the space shuttle program due to its resistance to saltwater corrosion. Natural tackiness, water washout resistance and load-carrying ability make HD Calcium Grease useful in large, low-speed, heavily loaded industrial antifriction bearings and slow-speed open gearing. HD Calcium Grease's calcium-sulfonate thickener is a gel or “nonsoap” grease type. This provides a grease which is resistant to oil bleeding, handles high temperatures (up to 500°F (260°C), 350°F (177°C) continuous), is shear stable and is nearly impervious to water washout. Rust and corrosion protection is good, particularly over long periods since water, air and other corrosive material cannot penetrate the gel structure of the grease as easily as with soap-thickened greases.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 9595Viscosity Index (Base Oil Property)
Saybolt Viscosity at 100°F 2177 SUS2177 SUSBase Oil Property
Saybolt Viscosity at 210°F 149 SUS149 SUSBase Oil Property
Kinematic Viscosity at 40°C (104°F) 470 cSt470 cStBase Oil
Kinematic Viscosity at 100°C (212°F) 31.5 cSt31.5 cStBase Oil
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Load Wear Index 4646
Four Ball Extreme Pressure, Weld Load 500 kg1100 lb (mass)
Four Ball Wear 0.460 mm0.0181 in
Penetration P(60), 1/10 mm 325325
Timken Test 15900 g35.0 lb
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 191 °C375 °F
Minimum Service Temperature, Air -12.2 °C10.0 °F
Pour Point -12.2 °C10.0 °F(Base Oil Property)
Dropping Point 288 °C550 °F
 
Descriptive Properties
ASTM Rust Fresh and SaltwaterPass
ColorTan-Brown
Copper Corrosion1B
Oil Separation0 wt.%
Roll Stability0.6% Change
ThickenerCalcium Sulfonate
Water Washout0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Phillips 66 HD Calcium Grease NLGI No. 2
Phillips 66 Tacna® HD Grease NLGI Grade 1
Morgan Advanced Ceramics Kaowool HD Organic RCF Vacuum Formed Thermal Ceramic

WCON209 / 75246

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.