MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

C-Glass Fiber, Generic
Categories: Ceramic; Glass; Glass Fiber; Oxide; Silicon Oxide; Other Engineering Material; Composite Fibers

Key Words: GRP composites, fiber glass composites, single fiber, FRP composites
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.52 - 2.56 g/cc0.0910 - 0.0925 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 3310 MPa480000 psi
 5380 MPa
@Temperature -190 °C
780000 psi
@Temperature -310 °F
Elongation at Break 4.8 %4.8 %
Modulus of Elasticity 68.9 GPa9990 ksi
Poissons Ratio 0.2760.276
Shear Modulus 27.0 GPa3920 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 6.9
@Frequency 1e+6 Hz
6.9
@Frequency 1e+6 Hz
Dissipation Factor 0.0085
@Frequency 1e+6 Hz
0.0085
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear  6.30 µm/m-°C
@Temperature 20.0 °C
3.50 µin/in-°F
@Temperature 68.0 °F
 6.30 µm/m-°C
@Temperature -30.0 - 250 °C
3.50 µin/in-°F
@Temperature -22.0 - 482 °F
Specific Heat Capacity  0.787 J/g-°C
@Temperature 23.0 °C
0.188 BTU/lb-°F
@Temperature 73.4 °F
 0.900 J/g-°C
@Temperature 200 °C
0.215 BTU/lb-°F
@Temperature 392 °F
Thermal Conductivity 1.10 W/m-K7.63 BTU-in/hr-ft²-°F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5331.533

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
D-Glass Fiber, Generic
A-Glass Fiber, Generic
E-Glass Fiber, Generic
S-2 Glass® Fiber
AR-Glass Fiber, Generic

CGF002 / 898

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.