MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Angst+Pfister APSOplast® PET-C Technical plastic
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: The specific properties of PET-C make this material particularly suited for mechanical precision and wearing parts.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0499 lb/in³DIN EN ISO 1183-1
Moisture Absorption 0.250 %0.250 %at saturation in standardized climate; DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8484DIN EN ISO 868
Ball Indentation Hardness 170 MPa24700 psiDIN EN ISO 2039-1
Tensile Strength, Yield 85.0 MPa12300 psi50 mm/min; DIN EN ISO 527
Elongation at Break 15 %15 %50 mm/min; DIN EN ISO 527
Modulus of Elasticity 3.00 GPa435 ksi1 mm/min; DIN EN ISO 527
Charpy Impact, Notched 0.200 J/cm²0.952 ft-lb/in²DIN EN ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohm1.00e+16 ohm
Dielectric Constant 3.43.4IEC 60250
Dielectric Strength 20.0 kV/mm508 kV/inIEC 60243
Dielectric Loss Index 0.00100.0010IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 60.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
33.3 µin/in-°F
@Temperature 73.4 - 140 °F
DIN 53752
Specific Heat Capacity 1.10 J/g-°C0.263 BTU/lb-°F
Thermal Conductivity 0.280 W/m-K1.94 BTU-in/hr-ft²-°F
Melting Point 255 °C491 °FISO 11357-3
Maximum Service Temperature, Air 115 °C239 °Fshort term
 180 °C356 °Flong term
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FDIN EN ISO 75/A
Minimum Service Temperature, Air -20.0 °C-4.00 °F
Flammability, UL94  HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 HB
@Thickness 6.00 mm
HB
@Thickness 0.236 in
 
Descriptive Properties
Colornatural (white), black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PANGP048 / 250546

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.