MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Changzhou Jinlibao JINLIBAO JLB-110805 Clear PETG face visor
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); PETG Copolyester

Material Notes:

Information provided by Changzhou Jinlibao Plastic Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 20.0 - 15000 microns0.787 - 591 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 60.0 MPa8700 psi
Elongation at Break >= 65 %>= 65 %
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.210 W/m-K1.46 BTU-in/hr-ft²-°F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 80 - 95 %80 - 95 %
 
Descriptive Properties
ColorClear, White, Green, Blue, Orange, Brown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Changzhou Jinlibao GETAILONG JLB-110900 Clear PETG sheet
Overview of materials for PETG Copolyester
Eastman Eastar 6763 PETG Copolyester
Eastman Eastar GN007 PETG Copolyester
Eastman Eastar GN071 Natural PETG Copolyester

PCHANG009 / 184985

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.