MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Exxtra™ Soft EMA6022 Molding Ethylene Methyl Acrylate, Molding Grade
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate; Ethylene-Methyl Acrylate Copolymer, Molding Grade

Material Notes: Exxtra™ Soft EMA6022 is an ethylene methyl acrylate copolymer that can be used as an impact modifier or compatibilizer in polymer compounds.It produces a soft, elastic film with good handling characteristics without additional additives. Exxtra™ Soft EMA6022 has been processed on typical LDPE compounding equipment at temperatures up to 625°F.

Availability: Latin America; North America

Additive: Antiblock: No; Slip: No; Thermal Stabilizer: Yes

Applications: Compatibilizer; Engineering thermoplastic impact modifier; Hot Melt Adhesives; Injection Molding; Masterbatch Base Resin; Soft, molded parts; Sound Deadening Foam

Information provided by ExxonMobil.

Key Words: Optema™ TC 121 Molding
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.943 g/cc0.0341 lb/in³ASTM D1505
Methyl Acrylate Content 21.5 %21.5 %ExxonMobil Method
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 84
@Time 15.0 sec
84
@Time 0.00417 hour
ASTM D2240
Hardness, Shore D 25
@Time 15.0 sec
25
@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 6.83 MPa990 psiASTM D638
Elongation at Break >= 500 %>= 500 %ASTM D638
Flexural Modulus, 1% Secant 35.2 MPa5100 psiASTM D790
Dart Drop, Total Energy  19.0 J
@Temperature 22.8 °C
14.0 ft-lb
@Temperature 73.0 °F
Instrumented; ASTM D3763
 23.0 J
@Temperature -40.0 °C
17.0 ft-lb
@Temperature -40.0 °F
Instrumented; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Melting Point 78.9 °C174 °FPeak; ExxonMobil Method
Vicat Softening Point 48.9 °C120 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEX98901 / 238283

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.