MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik 20C Pad Printing Strip Steel
Categories: Metal; Ferrous Metal; Special-Purpose Steel

Material Notes: The characteristics of Sandvik 20C strip steel are:
  • Excellent surface finish
  • Good flatness
  • Good etchability
  • High strength and wear resistance
  • Low level of non-metallic inclusions
  • Good dimensional tolerances
  • Information provided by Sandvik

    ASTM 1095; EN 1.1274

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength, Ultimate  1750 MPa
    @Diameter 0.475 - 0.600 mm
    254000 psi
    @Diameter 0.0187 - 0.0236 in
     1800 MPa
    @Diameter 0.475 - 0.600 mm
    261000 psi
    @Diameter 0.0187 - 0.0236 in
     1850 MPa
    @Diameter 0.425 - 0.475 mm
    268000 psi
    @Diameter 0.0167 - 0.0187 in
     1900 MPa
    @Diameter 0.375 - 0.425 mm
    276000 psi
    @Diameter 0.0148 - 0.0167 in
     1950 MPa
    @Diameter 0.275 - 0.375 mm
    283000 psi
    @Diameter 0.0108 - 0.0148 in
     2000 MPa
    @Diameter 0.225 - 0.275 mm
    290000 psi
    @Diameter 0.00886 - 0.0108 in
     2050 MPa
    @Diameter 0.175 - 0.225 mm
    297000 psi
    @Diameter 0.00689 - 0.00886 in
     2100 MPa
    @Diameter 0.125 - 0.175 mm
    305000 psi
    @Diameter 0.00492 - 0.00689 in

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    NSANDV283 / 19177

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.