MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Visico™ ME4425/LE4432 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Insulation  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Extruded

Material Notes: Visico ME4425/LE4432 is a black, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. ME4425 is a medium-density ethylene vinylsilane copolymer that offers improved deformation resistance, toughness and durability over convention low-density ethylene vinylsilane copolymers. The combination of a Visico base material, ME4425, and a tin catalyst masterbatch, LE4432, provides a highly scorch retardant compound with excellent thermal stability. ME4425/LE4432 contains a patented scorch retardant additive (SRA) that increases the processing window for a moisture crosslinking compound and minimizes the tendency for premature crosslinking in the extruder, head or die.

LE4424/LE4437 is recommended for use as insulation for low voltage control cables and power cables up to 6 kV in rating.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³ME 4425; ASTM D792
 1.05 g/cc0.0379 lb/in³LE 4432; ASTM D792
Melt Flow 0.70 g/10 min0.70 g/10 minME 4425; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield >= 18.6 MPa>= 2700 psiHeat Aging (7 days at 121°C); ASTM D412
 20.7 MPa3000 psiASTM D412
Elongation at Break <= 50 %<= 50 %Hot Creep Test (150°C, .2 MPa); ICEA T-28-562
 315 %315 %Heat Aging (7 days at 121°C); ASTM D412
 350 %350 %ASTM D412
Tensile Set <= 5.0 %<= 5.0 %Hot Creep Test (150°C,.2 MPa); ICE T-28-562
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.3
@Frequency 60 Hz
2.3
@Frequency 60 Hz
ASTM D150
Dielectric Strength >= 21.7 kV/mm>= 550 kV/inASTM D149
Dissipation Factor 0.00050
@Frequency 60 Hz
0.00050
@Frequency 60 Hz
ASTM D150
 
Processing PropertiesMetricEnglishComments
Middle Barrel Temperature >= 170 °C>= 338 °F
Front Barrel Temperature >= 170 °C>= 338 °F
Die Temperature >= 185 °C>= 365 °F
Head Temperature >= 185 °C>= 365 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total HP 401 MDPE, pipe, cable, sheet
Total Lacqtene® 2006 PBK 35 HDPE pipe, sheet
Syensqo (Solvay Specialty Polymers) Polidan® EC/MD Polyethylene, Crosslinked (XLPE)
Syensqo (Solvay Specialty Polymers) Polidan® EC/51 Polyethylene, Crosslinked (XLPE)
Syensqo (Solvay Specialty Polymers) Polidan® EC/110 Polyethylene, Crosslinked (XLPE)

PBOREA203 / 27510

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.