MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips 66 Omniguard® SRI ISO Grade 100 (with solvent)
Categories: Fluid; Lubricant; Calcium Gellant

Material Notes: Omniguard SRI is a multipurpose lubricant developed for the lubrication and preservation of wire ropes and cables and as a short-term corrosion preventive for metal parts and equipment exposed to wet or corrosive environments. Omniguard SRI is a calcium sulfonate grease fortified with special rust and corrosion inhibitors and diluted with a non-chlorinated solvent for ease of application. It may be applied by brush or spray. It is particularly recommended for use in applications where traditional asphaltic-type lubricants are not suitable.

Applications:

  • Wire ropes and wound cables on shovels, draglines, winches, boom trucks, cable cars and ski lifts
  • Corrosion preventive for equipment exposed to freshwater or saltwater, such as pumps and chains on offshore drilling rigs, ships and marine docks.
  • Corrosion preventive for metal parts, tools and other equipment in temporary storage or during shipment
Features/Benefit:
  • Outstanding rust and corrosion protection, including resistance to saltwater corrosion
  • Excellent wetting and penetrating ability for wire ropes and cables
  • Good low-temperature properties
  • Transparent for easy visibility
  • Easy to apply by brush or by spray
  • Excellent for protecting metal parts in temporary storage or during shipment

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.882 g/cc0.882 g/cc
Density 0.880 g/cc0.0318 lb/in³
Kinematic Viscosity at 40°C (104°F) 91.7 cSt91.7 cSt
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 250 kg551 lb (mass)ASTM D2596
Four Ball Wear 0.400 mm0.0157 inScar Diameter; ASTM D2266
 
Thermal PropertiesMetricEnglishComments
Pour Point -50.0 °C-58.0 °F
Flash Point >= 185 °C>= 365 °FCOC
 
Descriptive Properties
ColorTan-Brown
Copper Corrosion1aASTM D130
ThickenerCalcium Sulfonate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON5134 / 198387

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.