MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Resility ™ DPDB-3135 NT 7 MDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Molded; Medium Density Polyethylene (MDPE), Rotational Molded

Material Notes: Product Description: Resility™ DPDB-3135 NT 7 MDPE resin is produced via UNIPOL™ process technology from Dow and is intended for rotational and injection molding. It is specifically designed for applications requiring excellent processability and aesthetics combined with low warpage and good mechanical properties.
Processing and Stabilization: Resility ™ DPDB-3135 NT 7 MDPE resin is fully heat and UV stabilized resulting in a wide processing latitude, good color retention and long life expectancy.
  • Rotational molding or injection molding
  • For intermediate bulk containers, toys, general purpose custom molding, agricultural storage tanks, water tanks, marine parts, indoor consumer articles
  • Excellent impact strength, stress crack resistance and processability
  • Long term UV stabilization: UV-20+ stabilizer package
Complies with: FDA 21 CFR 177.1520 (a) 3.1a (with restrictions); EU No 10/2011; REACH; NSF51 and NSF 61; UL94 HB, UL746C f1

Availability: Latin America; North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: EU 2011/10/EC; FDA 21 CFR 177.1520 (a) 3.1a (with restrictions)

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ASTM D792
ESCR 100% Igepal® >= 1000 hour>= 1000 hourF50; ASTM D1693
Melt Flow 3.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 21.5 MPa3120 psiASTM D638
Elongation at Yield 13 %13 %ASTM D638
Flexural Modulus 0.745 GPa108 ksi1% Secant; ASTM D790B
Impact Test 255 J
@Thickness 6.35 mm,
Temperature -40.0 °C
188 ft-lb
@Thickness 0.250 in,
Temperature -40.0 °F
Rotational Molded
 
Thermal PropertiesMetricEnglishComments
Melting Point 126 °C259 °F
Deflection Temperature at 0.46 MPa (66 psi) 55.0 °C131 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 40.0 °C104 °FUnannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF556 / 311249

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.