MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemours Teflon™ 62N X Fine Powder PTFE Resin for Paste Extrusion
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Extruded

Material Notes: Teflon™ PTFE 62N X is a polytetrafluoroethylene fine powder resin used primarily for paste extrusion. Teflon™ PTFE 62N X offers the excellent combination of properties typical of Teflon™ fluoroplastic resins. Compared with other grades of PTFE fine powder, Teflon™ PTFE 62N X is a premium resin that has increased thermal stability, superior flex life, superior stress crack resistance, low permeability, and high clarity. Teflon™ PTFE 62N X is mainly used for tubing installed in demanding applications. It includes high performance articles, such as reinforced hose requiring the ultimate in reliability and performance in chemical, pharmaceutical, and automotive industry in use with hydraulic fluid, hydrocarbon fuel, or reactive gas. Such applications are, for example, over braided hoses for fuel assemblies and brake systems.

Information provided by Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.148 g/cc2.148 g/ccASTM D4895
Bulk Density 0.495 g/cc0.0179 lb/in³ASTM D4895
Water Absorption <= 0.010 %
@Time 86400 sec
<= 0.010 %
@Time 24.0 hour
ASTM D570
Particle Size 480 µm480 µmAverage; ASTM D4895
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 50 - 6550 - 65ASTM D2240
Tensile Strength 28.0 MPa4060 psiASTM D1457
Elongation at Break 400 %400 %ASTM D1457
Flexural Modulus 0.496 GPa71.9 ksiASTM D790
Flex Crack Resistance >= 1.00e+6>= 1.00e+6Cycles MIT Folding Endurance; ASTM D2176
Izod Impact, Notched 1.87 J/cm3.50 ft-lb/inASTM D256
Coefficient of Friction 0.050 - 0.100.050 - 0.10ASTM D1894
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+18 ohm-cm>= 1.00e+18 ohm-cmASTM D257
Surface Resistivity per Square >= 1.00e+18 ohm>= 1.00e+18 ohmASTM D257
Dielectric Constant 2.1
@Frequency 1e+6 Hz
2.1
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 18.0 kV/mm
@Thickness 0.100 mm
457 kV/in
@Thickness 0.00394 in
ASTM D149
Dissipation Factor <= 0.00010
@Frequency 1e+6 Hz
<= 0.00010
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance >= 300 sec>= 300 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Melting Point 322 °C612 °FSecond Peak; ASTM D4591
 327 °C621 °FASTM D3418
 341 °C646 °FInitial Peak; ASTM D4591
Flammability, UL94 V-0V-0
Oxygen Index >= 95 %>= 95 %ASTM D2863
 
Descriptive Properties
Chemical/Solvent ResistanceExcellentASTM D543
Detergent Resistance (hours)24On grit blast aluminum
 264
 624On aluminum
Extrusion Pressure (MPa)24ASTM D4895. @ RR= 400:1
Heat of Combustion5.1 MJ/kgASTM D240
Salt Spray Resistance Coatings (hours)192ASTM B117. 5% NaCl at 35 °C (95 °F). On aluminum.
 744+ASTM B117. 5% NaCl at 35 °C (95 °F).
Stretch Void Index<50ASTM D4895
Thermal Instability Index<7ASTM D4895
Weather Resistance (years unaffected)20Florida Exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDU8820 / 268746

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.