MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Goodfellow CVD Graphene Film on Quartz Glass
Categories: Carbon

Material Notes: State-of-the-art chemical vapor deposition (CVD) methods produce exceptionally high quality continuous monolayer (>95%) graphene film onto a variable thickness quartz glass for use as transparent conductors and in other innovative applications. The film may be transferred onto other substrates.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 10 - 30 µm10 - 30 µmDomain Size
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square <= 400 ohm<= 400 ohmvaries with dopant
 
Optical PropertiesMetricEnglishComments
Transmission, Visible >= 97 %>= 97 %
 
Descriptive Properties
Domain Size10 - 30 µm
Mobility> 3500 cm²/VsMax 17,000 cm²/Vs, varies with dopant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Goodfellow Ultra Clean CVD Graphene Film on SiO2/Si Wafers
Goodfellow CVD Graphene Film on PET
Goodfellow CVD Graphene Film on Copper Foil
Graphite, Carbon, C
Goodfellow Graphene Oxide (GO) Film

CGOODF095 / 187013

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.