MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Shell Carilon® DP R1130 Polyketone, 30% Glass Fiber Reinforced  (discontinued **)
Categories: Polymer; Thermoplastic; Polyketone; Polyketone, Glass Fiber Reinforced

Material Notes: Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON® Thermoplastic Polymer DP R1130 is a 30 percent glass fiber reinforced compound based on a developmental engineering polyketone resin available in natural and black from Shell Chemical Company. Due to the base polymer's balance of stiffness, toughness and chemical resistance coupled with its easy processing, this compound is expected to find application in the appliance, automotive, electrical and other industries.

Data provided by Shell Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.46 g/cc0.0527 lb/in³ASTM D792
Water Absorption 0.42 %0.42 %24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ASTM D785
Tensile Strength, Ultimate 130 MPa18900 psiASTM D638
Elongation at Break 3.1 %3.1 %ASTM D638
Tensile Modulus 8.30 GPa1200 ksiASTM D638
Flexural Strength 200 MPa29000 psiat 5% strain; ASTM D790
Flexural Modulus 7.20 GPa1040 ksiASTM D790
Izod Impact, Notched  0.850 J/cm
@Thickness 3.20 mm,
Temperature -40.0 °C
1.59 ft-lb/in
@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256
 1.40 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
2.62 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Taber Abrasion, mg/1000 Cycles 42421 kg load; CS-17 Wheel; ASTM D1044
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmASTM D257
Surface Resistance 1.00e+14 ohm1.00e+14 ohmASTM D257
Dielectric Constant  5.2
@Frequency 1e+6 Hz
5.2
@Frequency 1e+6 Hz
ASTM D150
 5.7
@Frequency 1000 Hz
5.7
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 24.0 kV/mm
@Thickness 1.60 mm
610 kV/in
@Thickness 0.0630 in
Short Term; ASTM D149
Dissipation Factor  0.012
@Frequency 1000 Hz
0.012
@Frequency 1000 Hz
ASTM D150
 0.040
@Frequency 1e+6 Hz
0.040
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 145 sec145 secASTM D495
Comparative Tracking Index 600 V600 VUL746A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 218 °C424 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 218 °C424 °FASTM D648
Vicat Softening Point 215 °C419 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 °C482 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Shell Carilon® DB6G6A10 Polyketone, 30% Glass-Reinforced General-Purpose Injection Molding Grade
Shell Carilon® DP P1000 Polyketone
Shell Carilon® DB6G6P30 Polyketone, Lubricated, Glass-Reinforced, Injection Molding Grade
Shell Carilon® DB6F1G30 Polyketone, Flame-Retarded, Tracking-Resistant, Glass-Reinforced Injection Molding Grade
RTP Company RTP 4505 TFE 15 Aliphatic Polyketone, Glass Fiber 30% - PTFE 15%

PCAR02 / 27911

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.