MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MAR-M432 Cast Nickel Superalloy
Categories: Metal; Superalloy; Nickel Base

Material Notes: Typical Applications: Integrally cast turbine wheels

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.16 g/cc0.295 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Rupture Strength  96.5 MPa
@Temperature 982 °C,
Time 3.60e+6 sec
14000 psi
@Temperature 1800 °F,
Time 1000 hour
As Cast
 138 MPa
@Temperature 982 °C,
Time 360000 sec
20000 psi
@Temperature 1800 °F,
Time 100 hour
As Cast
 331 MPa
@Temperature 816 °C,
Time 3.60e+6 sec
48000 psi
@Temperature 1500 °F,
Time 1000 hour
As Cast
 448 MPa
@Temperature 816 °C,
Time 360000 sec
65000 psi
@Temperature 1500 °F,
Time 100 hour
As Cast
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 2.8 %2.8 %
Boron, B 0.015 %0.015 %
Carbon, C 0.15 %0.15 %
Chromium, Cr 15.5 %15.5 %
Cobalt, Co 20 %20 %
Nickel, Ni 50 %50 %As Balance
Niobium, Nb (Columbium, Cb) 2.0 %2.0 %
Tantalum, Ta 2.0 %2.0 %
Titanium, Ti 4.3 %4.3 %
Tungsten, W 3.0 %3.0 %
Zirconium, Zr 0.050 %0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals INCONEL® Alloy 625
Special Metals NIMONIC® Alloy PK33
Special Metals INCONEL® Alloy 751
Special Metals INCONEL® Alloy 718
MAR-M918 Cobalt Alloy

NZ97026 / 191426

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.