MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECAFORM® AD HPV13 brown POM-H, PTFE Filled
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, PTFE-Filled

Material Notes:
  • very good slide and wear properties
  • good mechanical properties
  • good machinability
  • good chemical resistance
  • low water absorption
  • good dimensional stability
Target Industries:
  • food processing
  • food technology
  • conveyor technology
  • power engineering
  • gear manufacturing
  • packaging and paper machinery
  • business machines

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.50 g/cc0.0542 lb/in³
Moisture Absorption 0.120 %
@Time 86400 sec
0.120 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7878ASTM D 785
Hardness, Rockwell R 118118ASTM D 785
Tensile Strength, Yield 53.1 MPa7700 psiASTM D 638
Elongation at Break >= 10 %>= 10 %ASTM D 638
Modulus of Elasticity 2.62 GPa380 ksiASTM D 638
Flexural Strength 89.6 MPa13000 psiASTM D 790
Flexural Modulus 3.10 GPa450 ksiASTM D 790
Compressive Yield Strength 89.6 MPa
@Strain 10 %
13000 psi
@Strain 10 %
ASTM D 695
Compressive Strength 20.7 MPa
@Strain 1 %
3000 psi
@Strain 1 %
ASTM D 695
Compressive Modulus 1.65 GPa240 ksiASTM D 695
Izod Impact, Unnotched 0.801 J/cm1.50 ft-lb/inASTM D 256
Coefficient of Friction, Dynamic 0.12
@Pressure 0.276 MPa
0.12
@Pressure 40.0 psi
50 fpm; ASTM D 3702
Coefficient of Friction, Static 0.0700.070ASTM D 3702
K (wear) Factor 40.3 x 10-8 mm³/N-M20.0 x 10-10 in³-min/ft-lb-hrAgainst Steel, 40 psi, 50 fpm; ASTM D 3702
Limiting Pressure Velocity 0.0560 MPa-m/sec1600 psi-ft/min@ 100 fpm
 0.420 MPa-m/sec12000 psi-ft/min@ 10 fpm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 122 µm/m-°C68.0 µin/in-°FASTM D 696
Melting Point 119 °C247 °F
Maximum Service Temperature, Air 85.0 °C185 °FLong Term
Deflection Temperature at 0.46 MPa (66 psi) 168 °C334 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 118 °C244 °FASTM D 648
 
Descriptive Properties
Colorbrown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN8152 / 319080

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.