MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röchling LAMIGAMID® 710 High Density Polyethylene
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Cast

Material Notes: Application: chain-guides, cutting plates, liners

Information provided by Schwartz Technical Plastics GmbH. Schwartz was acquired by Röchling in 2018.

Key Words: HMW-PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.955 g/cc0.0345 lb/in³ISO R 1183
Moisture Absorption at Equilibrium 0.00 %0.00 %DIN 53473
Water Absorption at Saturation >= 0.10 %
@Temperature 20.0 °C
>= 0.10 %
@Temperature 68.0 °F
ISO R 62
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 36.0 MPa5220 psiHc 30; ISO 2039; partially
Tensile Strength, Yield 24.0 MPa3480 psiISO-DIS 527
Creep Strength 2.80 MPa406 psi1% elongation, 1000 h; DIN 53444
 4.50 MPa653 psi2% elongation, 1000 h; DIN 53444
Tensile Modulus 1.00 GPa145 ksiDIN 53457
Flexural Strength 31.0 MPa4500 psiDIN 54352
Flexural Modulus 0.900 GPa131 ksiDIN 53457
Izod Impact, Notched (ISO) 18.0 kJ/m²8.57 ft-lb/in²DIN 53453
Izod Impact Resistance NBNBswinging hammer 0,1 DIN 51222; DIN 53453
Coefficient of Friction 0.020 - 0.0800.020 - 0.080With lubrication
Coefficient of Friction, Dynamic 0.290.29no lube; Steel 2162, Rvst=2E-6m, p=0.05 Mpa, v=0.6 m/s, t=40°C
Tear Strength Test >= 8.0>= 8.0ISO-DIS 527
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmDIN 53482
Dielectric Constant 3.33.3DIN 53483
Dielectric Strength 50.0 kV/mm1270 kV/inDIN 53481
Dielectric Loss Index 0.000200.00020DIN 53483
 
Thermal PropertiesMetricEnglishComments
CTE, linear 200 µm/m-°C
@Temperature 20.0 - 100 °C
111 µin/in-°F
@Temperature 68.0 - 212 °F
DIN 53752
Specific Heat Capacity 2.30 J/g-°C0.550 BTU/lb-°F
Thermal Conductivity 0.140 W/m-K0.972 BTU-in/hr-ft²-°FDIN 52612
Melting Point 130 °C266 °FISO R 1218
Maximum Service Temperature, Air 80.0 °C176 °FContinuous
 120 °C248 °FIntermittent
Minimum Service Temperature, Air -100 °C-148 °FContinuous
 
Descriptive Properties
Creepage/leakage ResistanceKA3bDIN 53480
Friction Wear1 micron/km

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wefapress St 6000® XDP X-Ray Visible PE-UHMW
Okulen® 500 PE-HMW, Natural
Okulen® 500 PE-HMW, AST
Murtfeldt Original Material ”S”® Black Antistatic Polyethylene, Conductive
Murtfeldt Muralen® Polyethylene

PSCHW030 / 90227

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.