MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Spartech Royalite R60M Hi-Impact ABS/PVC Resin
Categories: Polymer; Thermoplastic; ABS Polymer; ABS/PVC Alloy; Vinyl (PVC)

Material Notes: Data provided by the manufacturer. This rigid, fire-rated, proprietary resin is specifically formulated to meet the requirements of the FAR 25.853 A flammability test. Primary applications are aircraft interior parts such as seat trim, trays and window surrounds.

Key Words: Poly(Acrylonitrile-Butadiene-Styrene); Polyvinyl Chloride
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ASTM D792
Water Absorption 0.030 %0.030 %24 hrs. ASTM D570
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inASTM D955
Melt Flow 3.9 g/10 min
@Load 5.00 kg,
Temperature 200 °C
3.9 g/10 min
@Load 11.0 lb,
Temperature 392 °F
Condition G; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9797ASTM D785
Tensile Strength, Yield 40.8 MPa5920 psiASTM D638
Modulus of Elasticity 2.20 GPa319 ksiASTM D638
Flexural Yield Strength 65.0 MPa9430 psiASTM D790
Flexural Modulus 2.40 GPa348 ksiASTM D790
Izod Impact, Notched 12.5 J/cm23.4 ft-lb/inASTM D256
 0.700 J/cm
@Temperature -20.0 °C
1.31 ft-lb/in
@Temperature -4.00 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 124 µm/m-°C
@Temperature 20.0 °C
68.9 µin/in-°F
@Temperature 68.0 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 72.0 °C162 °FAnnealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °C151 °FAnnealed; ASTM D648
Vicat Softening Point 70.0 °C158 °FASTM D1525
Flammability, UL94 V-0
@Thickness 0.711 mm
V-0
@Thickness 0.0280 in
Oxygen Index 36.8 %36.8 %ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Novatec Novaloy® 9000 PVC + ABS
Spartech Royalite R59M Hi-Impact ABS/PVC Resin
Overview of materials for ABS/PVC Alloy
S-Glass Fiber, Generic
Overview of materials for PVC, Molded

PROY32 / 66392

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.