MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Arkema Evatane® 1020 VB 2 Ethylene Vinyl Acetate
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate; Molded/Extruded

Material Notes: EVA copolymer made by high pressure tubular process. Applications Grade for transparent, resistant films, sealable at low temperature. Examples: laminates.

ISO data provided by the manufacturer, Arkema.

Key Words: EVAC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.925 g/cc0.0334 lb/in³
Melt Flow 2.63 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.63 g/10 min
@Load 4.76 lb,
Temperature 374 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 8.50 MPa1230 psi50 mm/min
Elongation at Break >= 50 %>= 50 %Nominal Strain; 50 mm/min
Tensile Modulus 0.140 GPa20.3 ksi1 mm/min
 
Thermal PropertiesMetricEnglishComments
Melting Point 104 °C219 °F10°C/min
Vicat Softening Point 84.0 °C183 °F50°C/hr; 50N
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 80 %80 %Mfr. reports 'Transparent' but doesn't quantify.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Evatane® 1020 VB 3 Ethylene Vinyl Acetate
Celanese Ateva® 1807EG Medical Grade EVA
Arkema Evatane® 1005 VN 4 Ethylene Vinyl Acetate
Arkema Evatane® 1005 VN 5 Ethylene Vinyl Acetate
Arkema Evatane® 1006 VL 2E Ethylene Vinyl Acetate

PARKG058 / 25534

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.