MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Silicone, RTV, Encapsulation Grade
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Encapsulation Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Encapsulation Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.710 - 3.20 g/cc0.0257 - 0.116 lb/in³Average value: 1.37 g/cc Grade Count:82
Water Absorption 0.0500 - 0.500 %0.0500 - 0.500 %Average value: 0.147 % Grade Count:7
Viscosity 50.0 - 880000 cP50.0 - 880000 cPAverage value: 23600 cP Grade Count:80
Linear Mold Shrinkage 0.00200 - 0.0200 cm/cm0.00200 - 0.0200 in/inAverage value: 0.00756 cm/cm Grade Count:17
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 13.0 - 87.013.0 - 87.0Average value: 49.9 Grade Count:64
 40.0 - 40.0
@Temperature 150 - 150 °C
40.0 - 40.0
@Temperature 302 - 302 °F
Average value: 40.0 Grade Count:1
Tensile Strength, Ultimate 0.310 - 6.86 MPa45.0 - 995 psiAverage value: 3.28 MPa Grade Count:59
Tensile Strength, Yield 1.17 - 1.72 MPa170 - 250 psiAverage value: 1.42 MPa Grade Count:3
Elongation at Break 15.0 - 400 %15.0 - 400 %Average value: 142 % Grade Count:52
Elongation at Yield 80.0 - 160 %80.0 - 160 %Average value: 110 % Grade Count:3
Penetration 5.00 - 3005.00 - 300Average value: 131 Grade Count:4
Penetration P(0), 1/10 mm 55.0 - 20055.0 - 200Average value: 103 Grade Count:3
Tear Strength Test 45.0 - 45.0
@Temperature 150 - 150 °C
45.0 - 45.0
@Temperature 302 - 302 °F
Average value: 45.0 Grade Count:1
Tear Strength 1.40 - 20.0 kN/m8.00 - 114 pliAverage value: 5.70 kN/m Grade Count:29
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+13 - 1.20e+16 ohm-cm1.00e+13 - 1.20e+16 ohm-cmAverage value: 9.40e+14 ohm-cm Grade Count:69
 1.00e+13 - 1.00e+13 ohm-cm
@Temperature 125 - 125 °C
1.00e+13 - 1.00e+13 ohm-cm
@Temperature 257 - 257 °F
Average value: 1.00e+13 ohm-cm Grade Count:1
Dielectric Constant 2.00 - 5.302.00 - 5.30Average value: 3.46 Grade Count:67
Dielectric Strength 7.40 - 27.0 kV/mm188 - 686 kV/inAverage value: 19.7 kV/mm Grade Count:71
Dissipation Factor 0.000100 - 0.07000.000100 - 0.0700Average value: 0.00975 Grade Count:72
 
Thermal PropertiesMetricEnglishComments
CTE, linear 1.40 - 730 µm/m-°C0.778 - 406 µin/in-°FAverage value: 223 µm/m-°C Grade Count:55
Thermal Conductivity 0.0159 - 140 W/m-K0.110 - 972 BTU-in/hr-ft²-°FAverage value: 4.34 W/m-K Grade Count:70
Maximum Service Temperature, Air 125 - 300 °C257 - 572 °FAverage value: 213 °C Grade Count:65
Minimum Service Temperature, Air -115 - -40.0 °C-175 - -40.0 °FAverage value: -64.7 °C Grade Count:60
Glass Transition Temp, Tg -110 - -40.0 °C-166 - -40.0 °FAverage value: -72.4 °C Grade Count:5
Flammability, UL94 HB - V-0HB - V-0Grade Count:17
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.39 - 1.421.39 - 1.42Average value: 1.41 Grade Count:15
Transmission, Visible 90.0 %90.0 %Average value: 90.0 % Grade Count:15
 
Processing PropertiesMetricEnglishComments
Processing Temperature 25.0 °C77.0 °FAverage value: 25.0 °C Grade Count:27
Cure Time 5.00 - 5760 min0.0833 - 96.0 hourAverage value: 1180 min Grade Count:29
 5.00 - 480 min
@Temperature 50.0 - 200 °C
0.0833 - 8.00 hour
@Temperature 122 - 392 °F
Average value: 82.5 min Grade Count:25
Pot Life 1.00 - 10100 min1.00 - 10100 minAverage value: 246 min Grade Count:65

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade
Overview of materials for Silicone Rubber
Elkem (Bluestar Silicones) BLUESIL™ RTV 3611 A/B Silicone Rubber
BASF Basotect G Foam
Overview of materials for Silicone Elastomer, for Thermal Management

O5201 / 78474

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.