MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Mid-Mountain Materials CERMEX® PR2200SW Thermal Insulation Mat
Categories: Ceramic; Glass; Glass Fiber; Oxide; Silicon Oxide; Other Engineering Material; Composite Fibers

Material Notes: Material: Alkaline Earth Silicate Wool
Construction: Paper, Organic Binder

Information provided by Mid-Mountain Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.176 - 0.224 g/cc0.00637 - 0.00810 lb/in³
Loss On Ignition 5.0 - 10 %5.0 - 10 %
Thickness 3125 microns123.0 mil
 6250 microns246 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 0.0345 - 0.0689 MPa5.00 - 10.0 psiFired Material
 0.414 - 0.621 MPa60.0 - 90.0 psiStandard Material
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0600 W/m-K
@Temperature 260 °C
0.416 BTU-in/hr-ft²-°F
@Temperature 500 °F
 0.0900 W/m-K
@Temperature 538 °C
0.625 BTU-in/hr-ft²-°F
@Temperature 1000 °F
 0.150 W/m-K
@Temperature 816 °C
1.04 BTU-in/hr-ft²-°F
@Temperature 1500 °F
 0.220 W/m-K
@Temperature 1093 °C
1.53 BTU-in/hr-ft²-°F
@Temperature 1999 °F
Melting Point >= 1300 °C>= 2370 °F
Maximum Service Temperature, Air 1200 °C2200 °FContinuous
 1260 °C2300 °FIntermittent
 
Component Elements PropertiesMetricEnglishComments
CaO 16 - 22 %16 - 22 %
MgO 12 - 19 %12 - 19 %
Other <= 1.0 %<= 1.0 %
SiO2 60 - 70 %60 - 70 %
 
Descriptive Properties
Al2O3 (%)Trace
ColorWhite
Fiber Index (%)60
Width (in)12
 24
 48

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parabeam Industrie Paraglass 3 3D Glass Fabric
NuSil MED-4086 Silicone, Low Consistency Elastomer - Restricted Medical Use
Mid-Mountain Materials CERMEX® PR1800SW Low Biopersistence Thermal Insulation Paper
Mid-Mountain Materials CERMEX® BK2200SW Low Biopersistence Thermal Insulation Blanket
Mid-Mountain Materials CERMEX® BK1800SW Low Biopersistence Thermal Insulation Blanket

CMID70 / 141238

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.