MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LATI Lapex R G/10 PPSU, 10% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³
Linear Mold Shrinkage, Flow 0.0045 - 0.0060 cm/cm0.0045 - 0.0060 in/in
Linear Mold Shrinkage, Transverse 0.0085 - 0.010 cm/cm0.0085 - 0.010 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  70.0 MPa
@Temperature 150 °C
10200 psi
@Temperature 302 °F
 80.0 MPa
@Temperature 120 °C
11600 psi
@Temperature 248 °F
 90.0 MPa
@Temperature 90.0 °C
13100 psi
@Temperature 194 °F
 100 MPa
@Temperature 60.0 °C
14500 psi
@Temperature 140 °F
 105 MPa
@Temperature 23.0 °C
15200 psi
@Temperature 73.4 °F
Elongation at Break  2.3 %
@Temperature 150 °C
2.3 %
@Temperature 302 °F
 2.5 %
@Temperature 120 °C
2.5 %
@Temperature 248 °F
 2.6 %
@Temperature 60.0 °C
2.6 %
@Temperature 140 °F
 2.6 %
@Temperature 90.0 °C
2.6 %
@Temperature 194 °F
 2.8 %
@Temperature 23.0 °C
2.8 %
@Temperature 73.4 °F
Tensile Modulus  3.40 GPa
@Temperature 150 °C
493 ksi
@Temperature 302 °F
 3.55 GPa
@Temperature 120 °C
515 ksi
@Temperature 248 °F
 3.70 GPa
@Temperature 90.0 °C
537 ksi
@Temperature 194 °F
 3.85 GPa
@Temperature 60.0 °C
558 ksi
@Temperature 140 °F
 4.00 GPa
@Temperature 23.0 °C
580 ksi
@Temperature 73.4 °F
Charpy Impact Unnotched 2.00 J/cm²9.52 ft-lb/in²
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 190 °C374 °F
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °F
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °F
Vicat Softening Point 220 °C
@Load 5.00 kg
428 °F
@Load 11.0 lb
Flammability, UL94  V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Oxygen Index 38 %38 %
 
Processing PropertiesMetricEnglishComments
Melt Temperature 350 - 390 °C662 - 734 °F
Mold Temperature 150 - 190 °C302 - 374 °F
Drying Temperature 140 - 180 °C
@Time 10800 sec
284 - 356 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Stat-Tech™ AT-CB2/000 CR Acetal (POM) Copolymer
Avient Edgetek® RA-10GF-10CF/000 HI Polyphenylsulfone (PPSU)
Avient Edgetek® PP-20GF/000 HS Polypropylene
BASF Ultrason® P 3010 PPSU Unreinforced Polyphenylsulfone
Ensinger RADEL® R-5500 Polyphenylsulfone (PPSU)

PLATH9617 / 177313

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.