MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Northstar Polymers MSB-D60A High Performance Polyurethane Cast Elastomer System
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Liquid

Material Notes: This is an Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires some lord bearing, high tensile strength, cut/tear resistance, dry-abrasion resistance, and low energy rebound/response. Ester base systems are generally less expensive than PTMEG base material. Possible applications for this material include buckets/flights for conveyers, abrasion resistance liners and parts, and other specialty parts. This is a conventional “full-prepolymer” type material cured with 1,4 BDO. Can be approved for FDA dry food contact.

Information provided by Northstar Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ASTM D2240
Tensile Strength 42.23 MPa6125 psiASTM D412
Elongation at Break 300 %300 %ASTM D412
Rebound 40 %40 %Bashore Rebound; ASTM D2632
Tear Strength 80.8 kN/m461 pliSplit; ASTM D624
 167 kN/m950 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 8585ASTM D4060
 
Processing PropertiesMetricEnglishComments
Processing Temperature 25.0 °C77.0 °FCuring Agent Temperature
 85.0 °C185 °FPrepolymer Temperature
Mold Temperature 100 °C212 °F
Cure Time  300 - 420 min
@Temperature 100 °C
5.00 - 7.00 hour
@Temperature 212 °F
De-mold Time
 480 min
@Temperature 82.2 °C
8.00 hour
@Temperature 180 °F
Complete Cure Cycle
Pot Life 0.750 min0.750 min
Gel Time 2.00 min2.00 min
 
Descriptive Properties
Curing AgentBNA-005
PrepolymerMSA-030
Weight Ratio1:0.143Prepolymer to Curing Agent Ratio

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BCC Products BC 8860 Polyurethane Elastomer
Polikim EFALON® K-35 PTFE, 35% Carbon Filled
Mearthane Durethane™ S DS-580D Solid Polyurethane Elastomer
BCC Products BC 8870 Polyurethane Elastomer
Adamas Adalon® 125 PTFE, 35% Carbon Filled

PNORTH09 / 54844

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.