MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Mid-Mountain Materials HYTEX® 1000 Fiberglass Industrial Textile
Categories: Ceramic; Glass; Glass Fiber; Other Engineering Material; Composite Fibers

Material Notes: Description: Hytex® is the trademark for the textile products manufactured by Mid-Mountain Materials, Inc. Hytex high performance textile products are manufactured from various yarns of varying chemistry and in differing configurations (cloth, tape, sleeving, rope etc.). Mid-Mountain can design hybrid materials by blending most any combination of yarns.

HYTEX® 1000 textiles are manufactured from fiberglass yam capable of resisting heat up to 1000ºF. Available as cloth, tape, sleeving, and rope, HYTEX® 1000 are either woven, knitted, or braided to meet a wide variety of end uses. HYTEX® 1000 fiberglass textile products provide the advantages of asbestos products without the risk of use. They will not burn, smolder, shrink, rot, or mildew. They have high dielectric strength, maintain a large measure of tensile strength at elevated temperatures, and are highly resistant to most chemicals.

Information provided by Mid-Mountain Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Melting Point 1120 °C2050 °F
Maximum Service Temperature, Air 538 °C1000 °FContinuous
 816 °C1500 °FShort Term
 
Descriptive Properties
Abrasion ResistanceFair
Acid ResistanceGood
Alkali ResistancePoor
ColorWhite
CompositionE-Glass
Solvent ResistanceExcellent
Sunlight & Aging ResistanceExcellent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Fiberglass Grade B
Mid-Mountain Materials HYTEX® 1400 Fiberglass Industrial Textile
Mitsubishi Chemical Advanced Materials TIVAR™ 1000 Virgin UHMW-PE, (Natural & Colors except Black)
E-Glass Fiber, Generic
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded

CMID00 / 1504

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.