MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Dowlex™ 2689G HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Product Description: Dowlex™ 2689G Polyethylene Resin is an ethylene-octene copolymer produced via INSITE™ Technology from Dow.
Main Characteristics: HDPE with excellent stiffness and processability
Complies with: (EU) No 10/2011; US FDA 21 CFR 177.1520© 3.1a
Consult the regulations for complete details.

Availability: North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: FDA 21 CFR 177.1520©3.1a; EU 10/2011

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.957 g/cc0.0346 lb/in³ASTM D792
Melt Flow 0.85 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.85 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 26.8 MPa3880 psiASTM D882
Film Tensile Strength at Yield, TD 26.6 MPa3860 psiASTM D882
Film Elongation at Break, MD 560 %560 %ASTM D882
Film Elongation at Break, TD 320 %320 %ASTM D882
2% Secant Modulus 0.814 GPa118 ksiMD; ASTM D882
 0.951 GPa138 ksiTD; ASTM D882
Elmendorf Tear Strength MD 16 g16 gMethod B; ASTM D1922
Elmendorf Tear Strength TD 350 g350 gMethod B; ASTM D1922
Dart Drop Test 66.0 g0.146 lbASTM D1709A
Film Tensile Strength at Break, MD 31.7 MPa4600 psiASTM D882
Film Tensile Strength at Break, TD 14.8 MPa2150 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 133 °C271 °F
 
Optical PropertiesMetricEnglishComments
Haze 48 %48 %ASTM D1003
Gloss 12 %
@Thickness 0.0508 mm
12 %
@Thickness 0.00200 in
45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 223 °C433 °F
Blow-up Ratio (BUR) 2.52.5
 
Descriptive Properties
Film Puncture Resistance49 ft-lb/in3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF421 / 311114

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.