MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LNP NORYL® MX5858 Polyphenylene Ether + Polystyrene, 34% Glass / Carbon / Mineral Reinforcement  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Glass + Mineral Filler

Material Notes: For use in IC Chip trays, electronic packaging.

  • Features: Electrically Conductive, High Heat Resistance
  • Forms: Pellets
  • Processing Method: Injection Molding
Information provided by LNP, a GE Plastics Company.

This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.29 g/cc1.29 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
@Thickness 3.18 mm
0.0050 - 0.0070 in/in
@Thickness 0.125 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 - 0.010 cm/cm
@Thickness 3.18 mm
0.0080 - 0.010 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 79.3 MPa11500 psiType I, 5 mm/min; ASTM D638
Tensile Strength, Yield 79.3 MPa11500 psiType I, 5 mm/min; ASTM D638
Elongation at Break 3.9 %3.9 %Type I, 5 mm/min; ASTM D638
Elongation at Yield 1.6 %1.6 %Type I, 5 mm/min; ASTM D638
Flexural Strength 119 MPa17300 psi50.8 mm Span, 1 mm/min; ASTM D790
Flexural Modulus 7.18 GPa1040 ksi(50.8 mm Span) 1mm/min; ASTM D790
Izod Impact, Notched 0.267 J/cm0.500 ft-lb/inASTM D256
Izod Impact, Unnotched 2.24 J/cm4.20 ft-lb/inASTM D256
Falling Dart Impact 8.25 J6.08 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+7 ohm-cm1.00e+7 ohm-cmASTM D257
Surface Resistance 1e+051e+05ASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 182 °C
@Thickness 3.18 mm
360 °F
@Thickness 0.125 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 174 °C
@Thickness 3.18 mm
345 °F
@Thickness 0.125 in
Unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 293 - 321 °C559 - 610 °F
Middle Barrel Temperature 299 - 327 °C570 - 621 °F
Front Barrel Temperature 299 - 335 °C570 - 635 °F
Nozzle Temperature 304 - 335 °C579 - 635 °F
Melt Temperature 304 - 335 °C579 - 635 °F
Mold Temperature 93.3 - 132 °C200 - 270 °F
Drying Temperature 110 - 121 °C230 - 250 °F
Dry Time 2 - 8 hour2 - 8 hour
Moisture Content 0.020 %0.020 %Suggested
Back Pressure 0.345 - 0.689 MPa50.0 - 99.9 psi
Shot Size 30 - 70 %30 - 70 %Suggested
Vent Depth 0.00380 - 0.00510 cm0.00150 - 0.00201 in
Screw Speed 50 - 100 rpm50 - 100 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PZLNP1380 / 51462

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.