MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trinseo CALIBRE™ 2091-15 Polycarbonate Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Gamma Radiation Resistant

Material Notes: Overview: CALIBRE™ MEGARAD™ 2091 Polycarbonate Resins are designed for single use medical devices (SUDs) that require gamma and electron-beam irradiation and an accelerated schedule for delivery of post-radiated products to customers – potentially 10 to 21 days sooner than currently available radiation-stabilized polycarbonate resins, depending on irradiation conditions. In addition, the resins are meant for applications that require a more water white appearance rather than the traditional purple tinted resin used to compensate for these sterilization methods. CALIBRE™ MEGARAD™ 2091-15 Polycarbonate resins has undergone biocompatibility texting based on ISO 10993 standards (Biological Evaluation of Medical Devices) and is suitable for use in approved medical applications.

Main Characteristics:

  • ISO 10993 (in progress)
  • Mold Release
  • Improved Color Compensation
Applications:
  • Medical Applications

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183/B; ASTM D792
Water Absorption 0.15 %
@Temperature 23.0 °C,
Time 86400 sec
0.15 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62; ASTM D570
Moisture Absorption at Equilibrium 0.32 %
@Temperature 23.0 °C
0.32 %
@Temperature 73.4 °F
50% RH; ISO 62; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inISO 294-4; ASTM D955
Melt Flow 15 g/10 min
@Load 1.20 kg,
Temperature 300 °C
15 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ISO 1133; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 118118ASTM D785
Tensile Strength at Break 68.0 MPa9860 psiISO 527-2/50
 68.3 MPa9910 psi50 mm/min; ASTM D638
Tensile Strength, Yield 62.0 MPa8990 psiISO 527-2/50
 62.1 MPa9010 psi50 mm/min; ASTM D638
Elongation at Break 150 %150 %50 mm/min; ASTM D638
Elongation at Yield 6.0 %6.0 %50 mm/min; ISO 527-2/50; ASTM D638
Tensile Modulus 2.30 GPa334 ksi50 mm/min; ISO 527-2/50; ASTM D638
Flexural Strength 96.5 MPa14000 psiMethod I (3 point load), 2.0 mm/min; ASTM D790
 98.0 MPa14200 psi3-point, 2.0 mm/min; ISO 178
Izod Impact, Notched 7.50 J/cm
@Temperature 23.0 °C
14.1 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Izod Impact, Notched (ISO) 75.0 kJ/m²
@Temperature 23.0 °C
35.7 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D256; ISO 180
Tensile Impact Strength 378 kJ/m²180 ft-lb/in²ASTM D1822
Dart Drop, Total Energy 81.3 J60.0 ft-lb3.39 m/sec; ASTM D3763
Abrasion 4545[%] Taber; ASTM D1044

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PZZDWST052 / 142261

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.