MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger DELRIN® 100AF natural blend POM-H, PTFE Filled
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, PTFE-Filled

Material Notes:
  • excellent wear properties
  • low static friction
  • high mechanical load capacity
  • good machinability
Target Industries:
  • conveyor technology
  • automotive industry
  • business machines
  • heavy duty industry
  • printing machines
  • packaging and paper machinery

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.50 g/cc0.0542 lb/in³
Moisture Absorption 0.120 %
@Time 86400 sec
0.120 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7979ASTM D 785
Tensile Strength, Yield 55.8 MPa8100 psiASTM D 638
Elongation at Break 10.3 %10.3 %ASTM D 638
Modulus of Elasticity 2.14 GPa310 ksiASTM D 638
Flexural Strength 87.6 MPa12700 psiASTM D 790
Flexural Modulus 3.34 GPa485 ksiASTM D 790
Compressive Yield Strength 86.2 MPa
@Strain 10 %
12500 psi
@Strain 10 %
ASTM D 695
Compressive Strength 8.27 MPa
@Strain 1 %
1200 psi
@Strain 1 %
ASTM D 695
Compressive Modulus 1.72 GPa250 ksiASTM D 695
 
Thermal PropertiesMetricEnglishComments
Melting Point 175 °C347 °FDIN EN ISO 11357
Maximum Service Temperature, Air 85.0 °C185 °FLong Term
 149 °C300 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 168 °C334 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 118 °C244 °FASTM D 648
 
Descriptive Properties
Colorbrown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN8133 / 319061

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.